The technology of an air purifier and nano-titanium dioxide is applied in the field of air purification, which can solve the problems of not being able to meet people's use needs, not being able to store for a long time, and secondary pollution of the environment, so as to prolong the effective use time, and the preparation method is simple and easy, and widely used Promoted app performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0011] The composite air purifier comprises the following raw materials in parts by mass: 5 parts of nano-titanium dioxide, 30 parts of activated carbon, 6 parts of stearic acid, and 50 parts of n-hexane.
[0012] The preparation method of the composite air purifier: according to the mass ratio, add stearic acid into n-hexane, stir at 55°C for 2 hours, add activated carbon, heat up to 65°C and reflux for 5 hours, add nano-titanium dioxide, and continue the reaction for 2 hours. , filtered and washed with n-hexane, and vacuum-dried at 40°C to constant weight to obtain the finished product of the present invention.
Embodiment 2
[0014] The composite air purifier comprises the following raw materials in parts by mass: 12 parts of nano-titanium dioxide, 35 parts of activated carbon, 8 parts of stearic acid, and 70 parts of n-hexane.
[0015] The preparation method of the composite air purifier: according to the mass ratio, add stearic acid into n-hexane, stir at 60°C for 2 hours, add activated carbon, heat up to 65°C and reflux for 4 hours, add nano-titanium dioxide, and continue the reaction for 2 hours. , filtered and washed with n-hexane, and vacuum-dried at 40°C to constant weight to obtain the finished product of the present invention.
Embodiment 3
[0017] The composite air purifier comprises the following raw materials in parts by mass: 10 parts of nano-titanium dioxide, 33 parts of activated carbon, 6.8 parts of stearic acid, and 60 parts of n-hexane.
[0018] The preparation method of the composite air purifier: according to the mass ratio, add stearic acid into n-hexane, stir at 58°C for 2 hours, add activated carbon, heat up to 65°C and reflux for 4.5 hours, then add nano-titanium dioxide, continue to react for 2 hours, and the reaction ends Afterwards, filter and wash with n-hexane, and vacuum-dry at 40°C to constant weight to obtain the finished product of the present invention.
[0019] The finished product that the present invention makes is used for the purification of the indoor air of 30 square meters of new houses, and this room is decorated before 5 days, and formaldehyde concentration is 15mg / m 3 , put 2g of the finished product of the present invention indoors, after 48 hours, measure the concentration of ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com