A substrate and camphor tree technology, applied in the field of seedling raising, can solve the problems of unsatisfactory three-phase structure of fertilizer retention, water retention and ventilation, untargeted seedling raising substrate, etc., achieving easy large-scale standardized production, and easy control of nutrient composition and content. , improve the absorption effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0024] A special matrix for raising camphor tree seedlings, comprising the following components in weight ratio: 82.5 parts of coconut fiber, 17 parts of multiple granulation agents, and 0.15 parts of humic acid, and the matrix is block-shaped. The multiple granulation agent includes the following components in weight ratio: 13 parts of acrylamide-acrylate copolymerized cross-linked product, 25 parts of acrylamide-sodium acrylate copolymer, 57 parts of montmorillonite, and chelated by the components combined. The acrylamide-acrylic acid salt copolymerized cross-linked product includes the following components in weight ratio: 65.5 parts of acrylamide, 23.5 parts of potassium acrylate, 9 parts of water, 0.75 parts of cross-linking agent, and through the copolymerization and cross-linking reaction of each component made. The acrylamide-sodium acrylate copolymer is formed by copolymerization of acrylamide and sodium acrylate. The English name of the cross-linking agent is: cr...
Embodiment 2
[0030] The components and production process of this embodiment are basically the same as those of Example 1, the difference lies in the content of each component of the matrix. The components contained therein and the weight ratio of each component are: 80 parts of coir fiber, 15 parts of multiple granulation agent and 0.1 part of humic acid. The multiple granulation agent includes the following components in weight ratio: 10 parts of acrylamide-acrylate copolymer cross-linked product, 20 parts of acrylamide-sodium acrylate copolymer, 55 parts of montmorillonite, and through the components The acrylamide-acrylic acid salt copolymerized cross-linked product includes the following components in weight ratio: 65 parts of acrylamide, 23 parts of potassium acrylate, 8 parts of water, and 0.5 part of a cross-linking agent.
Embodiment 3
[0032] The components and production process of this embodiment are basically the same as those of Example 1, the difference lies in the content of each component of the matrix. The components contained in it and the weight ratio of each component are: 85 parts of coir fiber, 20 parts of multiple granulation agent, and 0.2 part of humic acid. The multiple granulation agent includes the following components in weight ratio: 15 parts of acrylamide-acrylate copolymerized cross-linked product, 30 parts of acrylamide-sodium acrylate copolymer, 60 parts of montmorillonite, and the chelation by each component The acrylamide-acrylic acid salt copolymerized cross-linked product includes the following components in weight ratio: 66 parts of acrylamide, 24 parts of potassium acrylate, 10 parts of water, and 1.0 part of cross-linking agent.
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
height | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com