[0012] The preparation method of the light and thin non-glued cotton of this embodiment sequentially includes: material selection, opening, carding, oven baking, and molding and packaging.
[0013] Select 70wt% of polyester staple fiber and 30wt% of low-melting point fiber for batching, and then mix by multi-layer tiling method to mix and disperse different fibers; then send the mixed batching into the opener for opening, opening During the loosening process, the fibers are fully mixed and sent to the cotton box for storage after opening; then the opened fibers are fed from the cotton box to the carding machine for carding, and the feeding amount is controlled according to the product gram weight during carding, and Set the speed of the wool transmission chain to 8 m / min, and the frequency of reverse wool: 12 times / min, and the material is automatically fed through the cotton box, which is more conducive to mixing evenly and combing; then the carded fibers are laid directly thr...
Embodiment 2
[0015] The preparation method of the light and thin non-glued cotton of this embodiment sequentially includes: material selection, opening, carding, oven baking, and molding and packaging.
[0016] Select 80wt% of polyester staple fiber and 20wt% of low-melting point fiber for batching, and then mix by multi-layer laying method to mix and disperse different fibers; then send the mixed batching into the opener for opening, opening During the loosening process, the fibers are fully mixed and sent to the cotton box for storage after opening; then the opened fibers are fed from the cotton box to the carding machine for carding, and the feeding amount is controlled according to the product gram weight during carding, and Set the speed of the wool transmission chain to 15 m / min, and the frequency of reverse wool: 20 times / min, automatically feeding through the cotton box, which is more conducive to mixing evenly and combing; then the carded fibers are laid directly through the bridge...
Embodiment 3
[0018] The preparation method of the light and thin non-glued cotton of this embodiment sequentially includes: material selection, opening, carding, oven baking, and molding and packaging.
[0019] Select 90wt% of polyester staple fiber and 10wt% of low-melting point fiber for batching, and then mix by multi-layer tiling method to mix and disperse different fibers; then send the mixed batching into the opener for opening, opening During the loosening process, the fibers are fully mixed, and then sent to the cotton box for storage after opening; then the opened fibers are fed from the cotton box to the carding machine for carding. Set the speed of the wool transmission chain to 20 m / min, and the frequency of reverse wool: 25 times / min, automatically feeding through the cotton box, which is more conducive to mixing evenly and combing; then the carded fibers are laid directly through the bridge at one time The net enters the oven to bake, the temperature is 180 ℃, and the drying ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com