Pyraclostrobin water-dispersible granule and preparation method thereof
A technology of pyraclostrobin and dispersible granules, applied in the field of pesticides, can solve the problems of high use cost, endanger human health, environmental pollution and the like, and achieve the effects of saving packaging, reducing environmental pollution and reducing environmental pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] Example 1: 80% pyraclostrobin water dispersible granules.
[0034] Weigh 80% pyraclostrobin original powder, 4% sodium lauryl sulfate as wetting agent, 3% polycarboxylate as dispersant, 4% sodium lignosulfonate, 5% sodium sulfate as disintegrant, and sodium sulfate The foaming agent isooctyl alcohol 0.4%, the binder sucrose 0.5%, and the carrier kaolin is supplemented to 100%; the pyraclostrobin and other additives except the binder are mixed in a non-gravity mixer according to the formula ratio for 20 minutes , Then put the mixture into a double screw mixer (Ⅰ), and mix it with a jet mill to pulverize to a particle size of 1000 mesh or more, and collect it by a cyclone separator and a bag filter, and finally in a double screw mixer (Ⅱ) Mix it again for 30 minutes to obtain a uniform mother powder. Then accurately weigh the quantitative mother powder in the cyclone fluidized bed granulator, spray the binder aqueous solution according to the formula, and finally dry it to ...
Embodiment 2
[0035] Example 2: 50% pyraclostrobin water dispersible granules.
[0036] Weigh 50% pyraclostrobin original powder, 4% sodium lauryl sulfate as wetting agent, 3% naphthalene sulfonate formaldehyde condensate as dispersant, 4% sodium lignin sulfonate, and 30% disintegrant urea , Binder sucrose 0.5%, defoamer organic silicone 0.3%, carrier diatomaceous earth to make up to 100%, and pyraclostrobin and other additives except the binder in the non-gravity mixer according to the formula ratio After mixing for 20 minutes, put the mixture into the double screw mixer (Ⅰ), and pulverize by the jet mill while mixing to reach a particle size of more than 1000 meshes, collect it by a cyclone separator and a bag filter, and finally mix in the double screw Mix again for 30 minutes in the machine (II) to obtain a uniform master powder. Then accurately weigh a certain amount of mother powder in a rotary fluidized bed granulator, spray the binder aqueous solution according to the formula, and fin...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com