Inner wall coating composition with multiple environmental improvement functions
A technology for interior wall coatings and compositions, applied in antifouling/underwater coatings, coatings, paints containing biocide, etc., can solve the problems of high price of silver ions, poor long-term performance, single function, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0105] The preparation method of the interior wall paint with multiple environmental improvement functions of the present invention comprises the following steps:
[0106] The various components of the composition described in the first aspect above are mixed to obtain the interior wall paint with multiple environmental improvement functions.
[0107] In a specific embodiment, the interior wall paint with multiple environmental improvement functions is prepared by a method comprising the following steps:
[0108] a) Put the pure water into the dispersing tank, and control the speed at 700-800 rpm;
[0109] b) Slowly add the dispersant, wetting agent, defoamer, and thickener into the dispersion tank in turn for 15 minutes;
[0110] c) Then add various pigments and fillers in turn;
[0111] d) Then add the pH regulator and stir for 1 minute;
[0112] e) Then control the rotation speed at 1400-1500 rpm, and disperse for 20 minutes;
[0113] f) then add a small amount of pure ...
Embodiment 1~3
[0134] Prepare the raw materials for preparing the product of the present invention according to the weight percentages in Tables 1a-c.
[0135]
[0136]
[0137]
[0138]
[0139]
[0140]
[0141] First put pure water into the dispersing tank, and the speed is controlled at 800-1000 rpm; slowly add the dispersant, wetting agent, defoamer, and thickener into the dispersing tank for 15 minutes; then add various Pigments and fillers; then add PH regulator and stir for 1 minute; then control the speed at 1500-1800 rpm and disperse for 20 minutes; then add a small amount of pure water to cool down; then add film-forming substances; then add freeze-thaw stabilizer and bamboo charcoal particles; then add defoamer, antifungal agent, and preservative in the tank to disperse for 2 minutes; finally add pure water to adjust the viscosity to (100-102) KU, and then the finished product is made.
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
glass transition temperature | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com