Embodiment 1
[0012] A new type of straw composite fuel in this embodiment comprises the following raw materials by weight percentage: 40% of sewage treatment plant sludge, 40% of crop straw, 25% of coal powder, and 5% of coalification agent.
[0013] The 5% coalification agent contains: 0.5% sodium nitrate; 1.5% magnesium oxide; 0.4% calcium carbonate; 1% sodium hydroxide; 0.5% starch; 0.6% smoke suppressant, 0.5% sodium oxalate.
Embodiment 2
[0015] A new type of straw composite fuel in this embodiment comprises the following raw materials by weight percentage: 30% of sludge from a sewage treatment plant, 46% of crop straw, 20% of coal powder, and 4% of a coalification agent.
[0016] The 4% coalification agent contains: 0.6% sodium nitrate; 1% magnesium oxide; 0.1% calcium carbonate; 0.5% sodium hydroxide; 0.6% starch; 0.5% smoke suppressant, 0.7% sodium oxalate.
Embodiment 3
[0018] A new type of straw composite fuel in this embodiment comprises the following raw materials by weight percentage: 32% of sludge from a sewage treatment plant, 47% of crop straw, 13% of pulverized coal, and 8% of a coalification agent.
[0019] The 8% coalification agent contains: 0.8% sodium nitrate; 2% magnesium oxide; 0.2% calcium carbonate; 1% sodium hydroxide; 2% starch; 1.3% smoke suppressant, 0.7% sodium oxalate.
[0020] The preparation method of the straw composite fuel of the above-mentioned three embodiments, it comprises: according to the percentage by weight, the above-mentioned according to proportioning, the sludge of the raw material sewage treatment plant, crop straw, coal powder, coalification agent 1~5% 4 The raw materials are uniformly pulverized, stirred, and then placed for 5-8 days to recover, and then the molded fuel is produced; then it is baked and transformed at a baking temperature of 100-150 ° C, and air-dried for later use.
[0021] It has b...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com