A technology of benzotriazole and corrosion and scale inhibitor, which is applied in the field of high-efficiency and environment-friendly corrosion and scale inhibitor, can solve problems such as energy consumption, resource consumption, economic loss, etc., and achieves low equipment investment, increased coverage, Simple preparation process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] To prepare a composite corrosion and scale inhibitor containing benzotriazole, the materials are taken according to the following mass percentages: hydrolyzed polymaleic acid or styrene maleic acid 20% to 25%, acrylic acid-2-acrylamide-2- Methylpropanesulfonic acid 12%-18%, zinc nitrate or zinc sulfate 10%-15%, D-sodium gluconate or potassium gluconate 15%-20%, sulfamic acid 1%-2%, benzotriazepam 0.5% to 1% azole, the rest is distilled water; then distilled water, hydrolyzed polymaleic acid or styrene maleic acid, acrylic acid-2-acrylamide-2-methylpropanesulfonic acid, zinc nitrate or zinc sulfate, D- Add sodium gluconate or potassium gluconate, sulfamic acid and benzotriazole into the container in sequence according to the above, and stir at room temperature for 1 hour to obtain the product.
Embodiment 2
[0032] Prepare 100g of benzotriazole-containing composite corrosion and scale inhibitors, preparation process: get 50% hydrolyzed polymaleic acid 21g, 30% acrylic acid-2-acrylamide-2-methylpropanesulfonic acid 16g, Zn( NO 3 ) 2 .6H 2 O 14g, D-sodium gluconate 16, sulfamic acid 1.8g, benzotriazole 0.5g, and the rest are distilled water, which are successively added into a clean and dry beaker and stirred evenly to obtain the product.
Embodiment 3
[0034] Prepare 100g of benzotriazole-containing composite corrosion and scale inhibitors, preparation process: get 50% hydrolyzed polymaleic acid 22g, 30% acrylic acid-2-acrylamide-2-methylpropanesulfonic acid 15g, Zn( NO 3 ) 2 .6H 2 Add 13g of O, 17g of sodium D-gluconate, 1.7g of sulfamic acid, 0.6g of benzotriazole, and the rest in distilled water into a clean and dry beaker, and stir evenly to obtain the product.
PUM
Property | Measurement | Unit |
---|---|---|
hardness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com