Method for preparing embossed decorative veneer
A decorative sticker and process technology, applied in the field of sheet metal processing, can solve the problems of unnatural wood grain three-dimensional effect, unsatisfactory wire drawing effect, insufficient grain width, etc. The effect of workload
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment
[0027] Embodiment: the preparation method of a kind of embossment process decorative veneer of the present invention comprises the following steps:
[0028] (1) Selection. When logs enter the factory, avoid wood with cracked ends, choose denser stripes for patterns, and thicker stripes for straight grains;
[0029] (2) Hydrothermal softening, log cooking selects different temperatures according to the hardness and softness. The cooking temperature of soft wood is controlled at 60-80°C for 3-5 days; the temperature of hard wood is controlled at 90-100°C , time 7-10 days;
[0030] (3) Slicing. When slicing, the thickness of the veneer must be greater than or equal to 50 wires, and there are straight lines on both sides of the veneer, so that the joints can be spliced better and the joints are not obvious; the width of the veneer should be planed into 6 to 8 pieces. (that is, according to the width of the substrate, 6 to 8 veneers are veneered on a substrate) to reduce the num...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com