Method for making grass cloth into support of Chinese painting and calligraphy
A carrier, calligraphy and painting technology, applied in the field of making Chinese calligraphy and painting carriers, can solve the problems that it cannot be used as Chinese calligraphy and painting, and achieve the effect of facilitating calligraphy and painting, mounting and long-term preservation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] Embodiment 1: a kind of method that grass cloth is made into Chinese painting and calligraphy carrier, comprises the steps:
[0030] 1) Soaking: put the grass cloth in clear water, soak it at room temperature for 2 minutes, then remove and drain, wherein the weight ratio of the grass cloth to the water is 1:2;
[0031] 2) Extrusion and encryption dehydration: Roll the soaked linen under a pressure of 20 kg in an open width state, twist its warp and weft fibers into several densely arranged filaments, and the dehydrated linen contains The water content is 30%, and the slurry content is 25%;
[0032] 3) Drying: place the linen in open width, and dry at 45°C until the water content is 8%;
[0033] 4) Softening: Wrap the grass cloth on the surface of the roller, and roll it repeatedly for 2 minutes under a pressure of 20 kg to make a Chinese calligraphy and painting carrier.
Embodiment 2
[0034] Embodiment 2: a kind of method that grass cloth is made into Chinese calligraphy and painting carrier, comprises the steps:
[0035] 1) Soaking: Place the flat cloth of grass cloth in clear water, soak it for 20 minutes at room temperature, then remove and drain, wherein the weight ratio of grass cloth to clear water is 1:2;
[0036] 2) Extrusion and encryption dehydration: roll the soaked linen under a pressure of 40 kg in an open width state, twist its warp and weft fibers into several densely arranged filaments, and the dehydrated linen contains The water content is 20%, and the slurry content is 18%;
[0037] 3) Drying: place the linen cloth in open width, and dry it at room temperature until the water content is 6%;
[0038] 4) Softening: Wrap the grass cloth on the surface of the roller, and roll it repeatedly for 6 minutes under a pressure of 10 kg to make a Chinese calligraphy and painting carrier.
Embodiment 3
[0039] Embodiment 3: a kind of method that grass cloth is made into Chinese calligraphy and painting carrier, comprises the steps:
[0040] 1) Soaking: Place the flat cloth of grass cloth in clear water, soak it for 10 minutes at room temperature, then remove and drain, wherein the weight ratio of grass cloth to clear water is 1:2;
[0041] 2) Extrusion and encryption dehydration: roll the soaked grass cloth under a pressure of 30 kg in an open width state, twist its warp and weft fibers into several densely arranged filaments, and dehydrate the grass cloth The water content is 10%, and the pulp content is 13%;
[0042] 3) Drying: place the linen in open width, and dry at 45°C until the water content is 5%;
[0043] 4) Softening: Wrap the grass cloth on the surface of the roller, and roll it repeatedly for 5 minutes under a pressure of 15 kg to make a Chinese calligraphy and painting carrier, wherein, apply wax on the surface of the roller, and apply the wax evenly through the ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction