Microcrystalline Nitrocellulose Pyrotechnic Compositions
a technology of nitrocellulose and composition, which is applied in the direction of nitrocellulose explosive composition, explosives, weapons, etc., can solve the problems of inability of nitrocellulose to produce adequate colors, inability to generate sufficient temperature of pyrotechnic compositions including nitrocellulose as the sole propellant in color generating compositions, lack of functionality, etc., and achieve the effect of reducing toxic combustion products and smok
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Benefits of technology
Problems solved by technology
Method used
Examples
example 1
[0034] A blue star MCNC pyrotechnic composition comprised of: 87% microcrystalline nitrocellulose; 5% potassium nitrate; 4% copper oxide; and 4% hexachloroethane was dry mixed by hand and sieved several times to obtain a homogenous mixture. The homogenous mixture was then fed into a stokes rotary tablet press, and tablets of 0.21 inches in diameter by 0.21 inches tall were formed for use as star components by simple compression. The star components are at this point ready to be loaded into any desired fireworks device without further processing.
example 2
[0035] A red magnesium star MCNC pyrotechnic composition comprised of: 80% microcrystalline nitrocellulose; 10% strontium nitrate; 4% strontium carbonate; 3% magnesium metal powder; and 3% saran was dry mixed by hand and sieved several times to obtain a homogenous mixture. The homogenous mixture was then fed into a stokes rotary tablet press and tablets of 0.21 inches in diameter by 0.21 inches tall were formed by simple compression for use as star components. The star components are, at this point ready, to be loaded into any desired fireworks device without further processing.
example 3
[0036] A red flare MCNC pyrotechnic composition comprised of: 96% microcrystalline nitrocellulose and 4% strontium chloride was dry mixed by hand and sieved several times to obtain a homogenous mixture. The homogenous mixture was then incrementally consolidated by hydraulic press into a paper tube having an inside diameter of 0.5 inches and a length of 2.0 inches.
[0037] As various changes could be made in the above compositions without departing from the scope of the disclosure, it is intended that all matter contained in the above description or shown in the accompanying drawings shall be interpreted as illustrative and not in a limiting sense.
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com