Embodiment 1
[0024] (1) Dissolve 6.7 g of sodium carboxymethyl cellulose with 96 g of glycerol, then add 350 g of deionized water to make it swell;
[0025] (2) Add 30 g of sodium lauryl alcohol ether sulfate, 10 g of lauroyl diethanolamide, and 10 g of amine oxide respectively in 350 g of deionized water, and stir evenly;
[0026] (3) Put the product obtained in steps 1 and 2 in the stirring tank of the homogeneous emulsifier, raise the temperature to 55-65°C under ordinary stirring conditions, add 8.5g of hydrophilic lanolin and 15g of stearic acid, and stir evenly ; Then lower the temperature to 40-45°C, add 14g of hyaluronic acid, and stir evenly;
[0027] (4) Continue to add 320g of sodium chloride and 0.1g of essence, turn on the shearing and stirring function of the homogeneous emulsifier, set the shearing force to 1200rpm, and stir for 15 minutes, so that the sodium chloride can fully Dissolve, and achieve emulsification and homogeneity;
[0028] (5) Adjust the pH value to 5.5-8....
Embodiment 2
[0031] Repeat Example 1, with the following differences: in step 1, dissolve hydroxyethyl cellulose 8.5g with sorbitol 90g, then add deionized water 300g to make it swell; in step 2, add twelve Alkyl alcohol ether sodium sulfate 32g, lauroyl diethanolamide 12g, amine oxide 14g, and stir evenly; in step 3, the hydrophilic lanolin added is 7.0g, and in step 4, the sodium chloride added is 365g, Set the shear force to 700 rpm, and the stirring time to 22 minutes; the viscosity is 19000 mPa·s.
Embodiment 3
[0033] Repeat embodiment 1, following difference is arranged: in step 1, dissolve hydroxypropyl cellulose 7.5g with glycerol 90g, then add deionized water 320g and make it swell; In step 3, the hydrophilic lanolin that adds is 9.0g, the humectant is squalane 4.0g; in step 4, the sodium chloride added is 360g, the shear force is set to 800rpm, and the stirring time is 20 minutes; the viscosity is 25000mPa·s.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com