Sulfur-content-free odor additive for combustible gas, and preparation method thereof
A technology of sulfur content and additives, applied in gas fuel, gas/liquid distribution and storage, fuel and other directions, can solve the problems of deviation, self-polymerization, short shelf life, etc., and achieve sufficient supply, simple production process, and adsorption. small effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0033] A preparation method of an odor additive without sulfur content for combustible gas, comprising the following steps:
[0034] Step 1. Take 30-40 parts of methyl acrylate and 55-69 parts of ethyl acrylate and pump them into the enamel kettle by a centrifugal pump, stir at a normal speed, and control the temperature change. If the temperature is higher than 40°C, reduce the stirring speed to double Stirring time or suspend stirring and wait for the temperature to drop between 10-40°C.
[0035] Step 2. Add 1.0-5.0 parts of 2-ethyl-3-methylpyrazine liquid at a certain temperature, stir at a normal speed, and control the temperature change. If the temperature is higher than 40°C, reduce the stirring speed and double the stirring time, necessary Stirring can be suspended for ten minutes when the temperature drops to 10-40°C and then continue to stir.
[0036] Step 3. Add 0.05-0.15 parts of 2,6-di-tert-butyl-4-methylphenol solid at a certain temperature, stir at a normal spee...
Embodiment 1
[0045] Step 1. Take 39 parts of methyl acrylate and 59.8 parts of ethyl acrylate and pump them into the enamel kettle by centrifugal pump, and stir for 5 minutes.
[0046] Step 2. Control the temperature and add 1.0 parts of 2-ethyl-3-methylpyrazine liquid at 35°C, and stir for 5 minutes.
[0047] Step 3. Control the temperature at 35°C and add 0.1 part of 2,6-di-tert-butyl-4-methylphenol solid, and stir for 5 minutes.
[0048] Step 4. Control the temperature at 35°C and add 0.1 part of hydroquinone, and mix and stir for 30 minutes.
[0049] Step 5. The production process should be fully explosion-proof and fully enclosed; filling and discharging.
Embodiment 2
[0051] Step 1. Take 35 parts of methyl acrylate and 59.8 parts of ethyl acrylate and pump them into the enamel kettle by a centrifugal pump, and stir for 8 minutes.
[0052] Step 2. Control the temperature and add 5.0 parts of 2-ethyl-3-methylpyrazine liquid at 35°C, and stir for 8 minutes.
[0053] Step 3. Control the temperature at 35°C and add 0.1 part of 2,6-di-tert-butyl-4-methylphenol solid, and stir for 8 minutes.
[0054] Step 4. Control the temperature at 35°C and add 0.1 part of hydroquinone, and mix and stir for 40 minutes.
[0055] Step 5. The production process should be fully explosion-proof and fully enclosed; filling and discharging.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com