Spacer fluid for deepwater well cementation and preparation method thereof
A deepwater cementing and spacer fluid technology, applied in the direction of chemical instruments and methods, drilling compositions, etc., can solve the problems of poor isolation effect of drilling fluid and cement slurry, etc., to prevent mutual pollution, good compatibility, and facilitate construction Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0058] In the second aspect, the embodiment of the present invention also provides a method for preparing spacer fluid for deep-water well cementing, the method is applied to any spacer fluid for deep-water well cementing mentioned above, and the method includes:
[0059] According to the parts by weight of each component, the suspension stabilizer is added into the water, the first stirring is performed, and the first mixed liquid is obtained after dissolving.
[0060] Add diluent to the first mixed liquid, carry out the second stirring, after dissolving, add the weighting agent, carry out the third stirring, after uniform, obtain the spacer fluid for deep water well cementing.
[0061] Wherein, the suspension stabilizer is selected from at least one of attapulgite, bentonite, carboxymethyl cellulose, Wenlun gum, modified guar gum, polyacrylamide, and sodium silicate.
[0062] The above preparation method is simple, can be prepared on site, and is beneficial to deep water wel...
Embodiment 1
[0071] This example provides a spacer fluid for deepwater well cementing, which is prepared by the following method: add 2.85g attapulgite, 1.6g bentonite, 0.5g carboxymethyl cellulose, 0.05g modified melon to 100g water Er gum was stirred for 3 minutes at a speed of 4000 rpm, and dissolved for 30 minutes to obtain the first mixed solution. Then add 0.4g sodium lignosulfonate, 0.1g sulfonated tannin, 0.05g sodium chloride, 0.05g calcium chloride, 0.4g water to the first mixed solution, stir at 4000rpm for 10min, after uniform dissolution , to obtain the spacer fluid for deepwater well cementing provided in this embodiment.
Embodiment 2
[0073] This example provides a spacer fluid for deepwater well cementing, which is prepared by the following method: add 2.32g attapulgite, 1.28g bentonite, 0.36g carboxymethyl cellulose, 0.04g modified melon to 100g water Er gum was stirred for 3 minutes at a speed of 4000 rpm, and dissolved for 30 minutes to obtain the first mixed solution. Then add 0.8g sodium lignosulfonate, 0.2g sulfonated tannin, 0.1g sodium chloride, 0.1g calcium chloride, 0.8g water to the first mixed solution, stir at 4000rpm for 10min, after uniform dissolution , then add 28g of barite, stir at 4000rpm for 10min, and after uniformity, the spacer fluid for deepwater well cementing provided by this embodiment is obtained.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com