Embodiment 1
[0029] A water-resistant colored lead core, the components of the colored lead core and the contents of each component are: hexadecanoic acid 10%; wax 20%; organic pigment powder 18%; glue 8%; kaolin 44% %.
Embodiment 2
[0031] A production process for water-resistant colored lead cores, comprising the following steps:
[0032] Step 1, check whether the mixing mixer and high-temperature container are clean, and whether the valves are in place;
[0033] Step 2, put 20% hexadecanoic acid to octadecanoic acid, 15% wax and 2% glue into a high-pressure container, and melt at a high temperature of 80°C to obtain a melt mixture;
[0034] Step 3, 10% of organic pigment powder and 53% of talcum powder are put into a mixing mixer for stirring;
[0035] Step 4, stir for 5 minutes, after fully mixing the organic pigment powder and talcum powder, put the melt mixture of hexadecanoic acid, wax and glue melted in step 2 into the mixing mixer in step 3, Continue to stir, as the stirring continues, the raw materials in the mixing mixer gradually change from viscous to solid lumps;
[0036] Step 5: Put the raw materials after stirring in step 4 into the three-roller machine for extrusion. After extrusion, the...
Embodiment 3
[0040] A production process for water-resistant colored lead cores, comprising the following steps:
[0041] Step 1, check whether the mixing mixer and high-temperature container are clean, and whether the valves are in place;
[0042] Step 2, put 35% hexadecanoic acid to octadecanoic acid, 20% wax and 8% glue into a high-pressure container, and melt at a high temperature of 140°C to obtain a melt mixture;
[0043] Step 3, 18% talcum powder 19% of organic pigment powder is put into mixing mixer and stirs;
[0044] Step 4, stir for 3 minutes, after fully mixing the organic pigment powder and kaolin, put the molten mixture of hexadecanoic acid, wax and glue melted in step 2 into the mixing mixer in step 3, continue Stirring, as the stirring continues, the raw materials in the mixing mixer gradually change from viscous to solid lumps;
[0045] Step 5: Put the raw materials after stirring in step 4 into the three-roller machine for extrusion. After extrusion, the raw materials a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com