A method for improving the recovery rate of sulfur and gold in the tailings of old tailings ponds
A technology of tailings storage and recovery rate, applied in solid separation, flotation, etc., can solve the problems of high cost of flotation reagents and low recovery rate, and achieve the effects of reducing reagent costs, improving recovery rate, and saving resources
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] A method for improving the recovery rate of sulfur and gold in the tailings of old tailing ponds, specifically comprising the following steps:
[0013] A. Preparation of flotation pulp: Pour the tailings (sample) of an old tailing pond over 20 years into a plastic container, add water to make the pulp concentration 33%, stir evenly, and let it stand wet and soak for 24 hours to obtain Flotation pulp;
[0014] B. Aeration and stirring in the redox system: transfer the soaked flotation pulp from the plastic container to the tank of the inflatable flotation machine, add sodium sulfide solution to the flotation pulp, the dosage is 50 g / ton Sample, the mass concentration of sodium sulfide solution is 10%, the pulp in the flotation tank is aerated and stirred, the stirring time is 30 minutes, the impeller speed is 1800r / min, and the aeration volume is 1.2m 3 / h;
[0015] C. Sulfur-gold mineral flotation: add copper sulfate solution to the pulp flotation tank after inflating...
Embodiment 2
[0025] A method for improving the recovery rate of sulfur and gold in the tailings of old tailing ponds, specifically comprising the following steps:
[0026] A. Flotation pulp preparation: Pour the tailings (sample) of an old tailing pond over 40 years into a plastic container, add water to make the pulp mass concentration 33%, stir evenly, let stand wet and soak for 24 hours to obtain Flotation pulp;
[0027] B. Aeration and stirring in the redox system: transfer the soaked flotation pulp from the plastic container to the tank of the inflatable flotation machine, add sodium sulfide solution to the flotation pulp, the dosage is 100 g / ton Sample, the mass concentration of sodium sulfide solution is 10%, the pulp in the flotation tank is aerated and stirred, the stirring time is 40 minutes, the impeller speed is 2000r / min, and the aeration volume is 1.5m 3 / h;
[0028] C. Sulfur-gold mineral flotation: add copper sulfate solution to the pulp flotation tank after inflating and...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com