Method for improving formula of binding agent for sizing by using ethylene glycol phenyl ether
A technology of ethylene glycol phenyl ether and adhesives, which can be used in fiber processing, textiles and papermaking, and can solve the problems of environmental pollution, long starch grafting process, and high energy consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0009] Accurately weigh 30g of phosphate starch and 30g of acrylate solid slurry with an electronic balance and place them at the bottom of a 1L container. At the same time, weigh 1g of ethylene glycol phenyl ether solution into the container, add water to the container, and make the phosphate starch, acrylate , the total weight of ethylene glycol phenyl ether and water reaches 1kg, stir the solution evenly, heat the container in a water bath at 100°C, and at the same time use a stirrer to stir the mixed solution in the container, and set the stirring speed to 300 rpm / minute, stirring for 20 minutes, when the adhesive is completely gelatinized, stop stirring, seal the container with a film, and continue to cook the slurry in a water bath at 95-100°C for 40 minutes. Prepare an improved sizing adhesive, wind the prepared cotton roving on a special sizing frame, immerse the sizing frame in the adhesive for sizing, take it out after 5 minutes, and place it at 80°C Dry in the ove...
Embodiment 2
[0011] Accurately weigh 50g of phosphate starch and 50g of acrylate solid slurry with an electronic balance and place them at the bottom of a 1L container. At the same time, weigh 20g of ethylene glycol phenyl ether solution into the container, add water to the container, and make the phosphate starch, acrylate , the total weight of ethylene glycol phenyl ether and water reaches 1kg, stir the solution evenly, heat the container in a water bath at 100°C, and at the same time use a stirrer to stir the mixed solution in the container, and set the stirring speed to 300 rpm / minute, stirring for 20 minutes, when the adhesive is completely gelatinized, stop stirring, seal the container with a film, and continue to cook the slurry in a water bath at 95-100°C for 40 minutes. Prepare an improved sizing adhesive, wind the prepared cotton roving on a special sizing frame, immerse the sizing frame in the adhesive for sizing, take it out after 5 minutes, and place it at 80°C Dry in the ov...
Embodiment 3
[0013] Accurately weigh 40g of phosphate starch and 40g of acrylate solid slurry with an electronic balance and place them at the bottom of a 1L container. At the same time, weigh 10g of ethylene glycol phenyl ether solution into the container, add water to the container, and make the phosphate starch, acrylate , the total weight of ethylene glycol phenyl ether and water reaches 1kg, stir the solution evenly, heat the container in a water bath at 100°C, and at the same time use a stirrer to stir the mixed solution in the container, and set the stirring speed to 300 rpm / minute, stirring for 20 minutes, when the adhesive is completely gelatinized, stop stirring, seal the container with a film, and continue to cook the slurry in a water bath at 95-100°C for 40 minutes. Prepare an improved sizing adhesive, wind the prepared cotton roving on a special sizing frame, immerse the sizing frame in the adhesive for sizing, take it out after 5 minutes, and place it at 80°C Dry in the ov...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com