[0016] An environment-friendly water-based varnish, comprising the following raw materials in weight percentage: 45% water-based acrylic resin, 20% water-based alkyd resin, 24% acrylic emulsion, 7% auxiliary solvent, 1% leveling agent, and 1% wetting agent , 1% defoamer, 1% wear agent. The auxiliary solvent in this embodiment is formed by mixing water and isopropanol in a ratio of 1:1.
[0017] The preparation method of this embodiment includes the following steps: according to the weight percentage and under a water bath at 30°C, mix the water-based acrylic resin, the water-based alkyd resin and the auxiliary solvent together, after stirring evenly, add the acrylic emulsion while stirring , continue to stir for 30 minutes, add leveling agent, wetting agent, defoamer, wear-resistant agent, and stir for 50 minutes.
Embodiment 2
[0019] An environment-friendly water-based varnish, comprising the following raw materials in weight percentage: 35% water-based acrylic resin, 29% water-based alkyd resin, 20.2% acrylic emulsion, 15% auxiliary solvent, 0.2% leveling agent, and 0.2% wetting agent , 0.2% defoamer, 0.2% wear agent. The auxiliary solvent in this embodiment is formed by mixing water and isopropanol in a ratio of 1:1.
[0020] The preparation method of this embodiment includes the following steps: according to the weight percentage and under a water bath at 20°C, mix the water-based acrylic resin, the water-based alkyd resin and the auxiliary solvent together, after stirring evenly, add the acrylic emulsion while stirring After continuing to stir for 20 minutes, add leveling agent, wetting agent, defoamer, wear-resistant agent, and stir for 40 minutes.
Embodiment 3
[0022] An environment-friendly water-based varnish, including the following raw materials in weight percentage: 38% water-based acrylic resin, 28% water-based alkyd resin, 22% acrylic emulsion, 10% auxiliary solvent, 0.5% leveling agent, 0.5% wetting agent , 0.5% defoamer, 0.5% wear agent. The auxiliary solvent in this embodiment is formed by mixing water and isopropanol in a ratio of 1:1.
[0023] The preparation method of this embodiment includes the following steps: according to the weight percentage and under a water bath at 25°C, mix the water-based acrylic resin, the water-based alkyd resin and the auxiliary solvent together, after stirring evenly, add the acrylic emulsion while stirring After continuing to stir for 25 minutes, add leveling agent, wetting agent, defoamer, wear-resistant agent, and stir for 45 minutes.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com