A printing process for mobile phone glass panel
A glass panel and mobile phone technology, applied in printing, printing devices, etc., can solve the problems of low product yield, poor light-shielding performance, poor adhesion ability, etc., achieve excellent adhesion performance, enhance the light-shielding effect, and improve the light-shielding effect Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0043] A printing process for a glass panel of a mobile phone is to perform multiple bottom cover printing on the back of the glass panel, which specifically includes the following steps:
[0044] Step 1. The first white background printing: the first white background printing layer is printed on the back of the glass panel of the mobile phone by screen printing. The printing materials required by weight are: 100 parts of ink, 9 parts of curing agent and thinner 4 copies, the screen mesh number of the screen printing is 400 meshes, the hardness of the squeegee board is 75A, the curing temperature is 145°C, the curing time is 35 minutes, and the overall thickness of the ink after printing is 6μm.
[0045] Step 2. The second white background printing: the second white background printing layer is printed on the first white background printing layer. The printing materials required by weight are: 100 parts of ink, 8 parts of curing agent and 3 parts of diluent , The screen mesh of the...
Embodiment 2
[0049] A printing process for a glass panel of a mobile phone is to perform multiple bottom cover printing on the back of the glass panel, which specifically includes the following steps:
[0050] Step 1. The first white background printing: the first white background printing layer is printed on the back of the glass panel of the mobile phone by screen printing. The printing materials required by weight are: 100 parts of ink, 8 parts of curing agent and thinner 3 copies, the screen mesh number of the screen printing is 420, the hardness of the squeegee board is 80A, the curing temperature is 140°C, the curing time is 40 minutes, and the overall thickness of the ink after printing is 7μm.
[0051] Step 2. The second white background printing: the second white background printing layer is printed on the first white background printing layer. The printing materials required by weight are: 100 parts of ink, 9 parts of curing agent and 4 parts of diluent , The screen mesh of the screen...
Embodiment 3
[0055] A printing process for a glass panel of a mobile phone is to perform multiple bottom cover printing on the back of the glass panel, which specifically includes the following steps:
[0056] Step 1. The first white background printing: the first white background printing layer is printed on the back of the glass panel by screen printing. The materials required for printing are: 100 parts of ink, 10 parts of curing agent and 4 parts by weight. The screen printing screen mesh is 450 meshes, the hardness of the squeegee is 70A, the curing temperature is 150°C, the curing time is 25 minutes, and the thickness of the printing ink is 7μm.
[0057] Step 2. The second white background printing: the second white background printing layer is printed on the first white background printing layer. The materials required for printing are: 100 parts of ink, 10 parts of curing agent and 4 parts by weight. The screen printing screen mesh number is 370 meshes, the hardness of the squeegee is 8...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com