A water-based whiteboard wall paint
A whiteboard and wall paint technology, applied in the field of wall paint, can solve problems such as unsatisfactory customers, non-environmental protection of paint, and peeling off in flakes, and achieve the effects of meeting environmental protection requirements, reducing solvent emissions, and being easy to operate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A water-based whiteboard wall paint, comprising component A and component B, the component A and component B are mixed at a mass ratio of 1:3-6, and stirred evenly. The component B includes by mass parts: 22.00-38.00 mass parts of modified amine curing agent, 24.00-36.00 mass parts of water, 0.2-0.8 mass parts of dispersant, 0-3.20 mass parts of coupling agent, 0-3.00 mass parts of thixotropic agent 0.60 parts by mass, 26.00-44.00 parts by mass of pigment extender, 0.40-1.00 parts by mass of leveling agent, and 0.10-0.40 parts by mass of surfactant. The component A includes in parts by mass: 68.00-84.00 parts by mass of modified epoxy resin, 8.00-17.00 parts by mass of diluent, 6.00-11.00 parts by mass of surfactant, and 1.00-5.00 parts by mass of accelerator.
[0026] The preparation method of above-mentioned component B obtains according to the following steps:
[0027] Step 1. After adding modified amine curing agent, water, dispersant, coupling agent and thixotropi...
Embodiment 2
[0035] A water-based whiteboard wall paint, comprising component A and component B, the component A and component B are mixed at a mass ratio of 1:3, and stirred evenly. The component B includes in parts by mass: 38.00 parts by mass of a modified amine curing agent, 32.00 parts by mass of water, 0.20 parts by mass of a dispersant, 0.0 parts by mass of a coupling agent, 0.40 parts by mass of a thixotropic agent, and 26.00 parts by mass of an extender pigment, 1.0 parts by mass of leveling agent, 0.4 parts by mass of surfactant. The component A includes, in parts by mass: 68.00 parts by mass of modified epoxy resin, 17.00 parts by mass of diluent, 11.00 parts by mass of surfactant, and 4.00 parts by mass of accelerator.
[0036] The preparation method of above-mentioned component B obtains according to the following steps:
[0037] Step 1. After adding modified amine curing agent, water, dispersant, coupling agent and thixotropic agent in sequence, disperse at a medium speed of...
Embodiment 3
[0045] A water-based whiteboard wall paint, comprising component A and component B, the component A and component B are mixed at a mass ratio of 1:5, and the mixture is uniformly stirred. The component B includes in parts by mass: 32.00 parts by mass of a modified amine curing agent, 32.00 parts by mass of water, 0.30 parts by mass of a dispersant, 1.0 parts by mass of a coupling agent, 0.20 parts by mass of a thixotropic agent, and 34.00 parts by mass of an extender pigment, 0.40 parts by mass of the leveling agent, and 0.10 parts by mass of the surfactant. The component A includes in parts by mass: 84.00 parts by mass of modified epoxy resin, 8.00 parts by mass of diluent, 7.00 parts by mass of surfactant, and 1.00 parts by mass of accelerator.
[0046] The preparation method of above-mentioned component A obtains according to the following steps:
[0047] Step 1. After adding modified amine curing agent, water, dispersant, coupling agent and thixotropic agent in sequence, ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com