Low-grade fluorite silicon reduction mineral processing process
A low-grade, high-tech technology, applied in the direction of flotation, solid separation, etc., can solve the problems of no inhibitor application introduction, etc., and achieve the effect of being conducive to selection and removal of impurities, enhanced defoaming effect, and easy control
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] 1) Rough separation: After the ore is crushed, it enters the ball mill for grinding to form a slurry, and Na is added during the grinding process. 2 CO 3 , sodium silicate to adjust the pulp, add oleic acid in the mixing tank to adjust the pulp, and then use the flotation machine for rough separation, the foam product produced by flotation is concentrated ore, which enters the selection process, and the remaining products enter the sweeping process as medium ore , the tailings produced by sweeping are pumped into the tailings dam by the tailings pump;
[0019] 2) The first beneficiation: the first beneficiation of the rough-selected concentrate is carried out with a flotation machine, the produced concentrate enters the regrinding process, and the middle ore returns to the upper-level flotation operation;
[0020] 3) Regrinding process: the concentrate after primary refining enters the ball mill for regrinding. In order to increase the monomer dissociation degree of fl...
Embodiment 2
[0023] Embodiment 2: the difference with embodiment 1 is:
[0024] The sulfuric acid, water glass and oxalic acid in the inhibitor are diluted respectively to reach 6%, 6% and 9% respectively, and then mixed according to the volume ratio of 1:2:2.
[0025] This method is suitable for low-grade fluorspar mines with less mud content.
Embodiment 3
[0026] Embodiment 3: the difference with embodiment 1 is:
[0027] The sulfuric acid, water glass and oxalic acid in the inhibitor are diluted respectively to reach 9%, 5.5% and 5.5% respectively, and then mixed according to the volume ratio of 1:2:2.
[0028] This method is suitable for low-grade fluorspar mines with high quartz content and close symbiotic relationship.
[0029] The configuration steps of the above inhibitors: first dilute sulfuric acid, water glass, and oxalic acid as required, then put 1 volume of dilute sulfuric acid solution in a container, then pour 2 volumes of water glass solution into sulfuric acid, and stir for 2 minutes , and finally pour 2 volumes of oxalic acid solution into the above mixed solution and stir for 2 minutes.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com