Embodiment 1
[0014] Such as figure 1 As shown, the sludge with a moisture content of 80% is mixed with pyrite, wherein the mixed pyrite accounts for 10% of the total weight, and then the mixture is sent into the mixer, and the mixer adopts a double-shaft counter-rolling mixer. Add dry sludge with a moisture content of 5% while stirring, and temper the sludge to a sludge with a moisture content of 30.9%. After obtaining 30.9% sludge, part of the sludge is dried to obtain sludge with a moisture content of 5%. The mud returns to the stirring and tempering stage. The remaining 30.9% of the sludge is discharged for further treatment, such as brick making and other comprehensive utilization processes.
Embodiment 2
[0016] Add pyrite into sludge with a moisture content of 75%, wherein the mixed pyrite accounts for 40% of the total weight, and add dry mud with a moisture content of 7% while stirring, and temper the sludge to a moisture content of It is 35.0% sludge. After obtaining 35.0% sludge, part of the sludge is dried to obtain sludge with a moisture content of 7%, and then returns to the stirring and tempering stage. The remaining 35.0% of the sludge is discharged for further treatment, such as brick making and other comprehensive utilization processes.
Embodiment 3
[0018] Mix the fly ash into the sludge with a water content of 70%, wherein the mixed fly ash accounts for 2% of the total weight, and then send the mixture into the mixer. The mixer adopts a double-shaft counter-rolling mixer. Add dry sludge with a moisture content of 8%, and temper the sludge to a sludge with a moisture content of 32.3%. After obtaining 32.3% sludge, part of the sludge is dried to obtain dry sludge with a moisture content of 8%, and then return Stirring and tempering phase. The remaining 32.3% of the sludge is discharged for further treatment, such as brick making and other comprehensive utilization processes.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com