A clay acid reducing agent and active technology, which is applied in other chemical processes, silicon compounds, chemical instruments and methods, etc., can solve the problems of large water consumption for acid and affect product quality, etc., and achieve simple production process and simplified production process , the effect of reducing the water consumption of acid washing
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Example Embodiment
[0043] Example 1.
[0044] The first active clay acid reducing agent, which is composed of the following ingredients in weight percentage: SiO 2 Content 36.12%, Al 2 O 3 Content 19.26%, Fe 2 O 3 The content is 8.58%, MgO content is 9.86%, CaO content is 10.26%, K 2 O content 4.0%, TiO 2 Content 1.2%, Na 2 The O content is 7.65%, other impurities are 3.07%, and the PH value is 7.2.
[0045] The first preparation method of activated clay acid reducing agent includes the following steps:
[0046] Step 1: Raw material selection, select 90 parts of gray attapulgite, 5 parts of bentonite, 3 parts of kaolinite, 1 part of illite and 1 part of quartz as basic raw materials, and make granular materials;
[0047] Step 2: Mix the raw materials, mix the gray attapulgite, bentonite, kaolinite, illite and quartz in step one to form Mixture A;
[0048] Step 3: Acidification treatment, use 3 parts of 38% hydrochloric acid and 15 parts of water for the mixture A in step 2 to be acidified at room temperat...
Example Embodiment
[0056] Example 2.
[0057] The second activated clay acid reducing agent is composed of the following ingredients in weight percentage: SiO 2 Content 59.62%, Al 2 O 3 Content 14.53%, Fe 2 O 3 Content 2.82%, MgO content 9.17%, CaO content 5.26%, K 2 O content 0.17%, TiO 2 Content 2.39%, Na 2 O content is 4.45%, other impurities are 1.59%, PH value is 8.4.
[0058] The second preparation method of activated clay acid reducing agent includes the following steps:
[0059] Step 1: Raw material selection, select 90 parts of gray-green attapulgite, 5 parts of bentonite, 2 parts of kaolinite, 2 parts of quartz and 1 part of dolomite as basic raw materials, and make granular materials;
[0060] Step 2: Mix the raw materials, mix the gray-green attapulgite, bentonite, kaolinite, quartz and dolomite in step one to form Mixture A;
[0061] Step 3: Acidification treatment, the mixture A in step 2 is acidified at room temperature with 5 parts of 36% hydrochloric acid and 15 parts of water to form mix...
Example Embodiment
[0069] Example 3.
[0070] The third activated clay acid reducing agent is composed of the following components in weight percentage: SiO 2 47.62% content, Al 2 O 3 Content 9.53%, Fe 2 O 3 The content is 0.82%, MgO content is 9.17%, CaO content is 4.26%, K 2 O content 0.19%, TiO 2 Content 2.64%, Na 2 O content is 3.45%, other impurities 22.32%, PH value is 7.6.
[0071] The third preparation method of activated clay acid reducing agent includes the following steps:
[0072] Step 1: Raw material selection, select 90 parts of off-white attapulgite, 5 parts of bentonite, 3 parts of kaolinite, 1 part of quartz and 1 part of feldspar as basic raw materials, and make granular materials;
[0073] Step 2: Mix the raw materials, mix the off-white attapulgite, bentonite, kaolinite, quartz and feldspar in step one to form Mixture A;
[0074] Step 3: Acidification treatment, the mixture A in step 2 is acidified with 10 parts 37% hydrochloric acid and 15 parts water at room temperature to form mixtu...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com