Willow weaving paint
A technology of alkyd paint and water-based acrylic, applied in the field of paint, can solve the problems of user's health impact, short storage time, poor adhesion, etc., and achieve the effect of fast drying, low cost and strong adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] A kind of willow paint, made by the following components by weight: 20 parts of water-based acrylic resin, 35 parts of water, 14 parts of water-soluble alkyd paint, 2 parts of manganese dioxide, 6 parts of calcium stearate, 5 parts of three Glyceryl stearate, 16 parts of acrylic acid emulsion, 3 parts of sodium dodecyl sulfonate, 6 parts of sodium metaphosphate, 2 parts of pentaerythritol, 2 parts of auxiliary agent, the auxiliary agent is calculated by weight percentage: 30% attapulgite Soil, 30% epoxy resin, 40% starch.
Embodiment 2
[0012] A kind of willow paint, made of the following components by weight: 20 parts of water-based acrylic resin, 35 parts of water, 12 parts of water-soluble alkyd paint, 2 parts of manganese dioxide, 5 parts of calcium stearate, 4 parts of three Glyceryl stearate, 15 parts of acrylic acid emulsion, 3 parts of sodium dodecyl sulfonate, 6 parts of sodium metaphosphate, 2 parts of pentaerythritol, 2 parts of auxiliary agents, the auxiliary agent is calculated as: 30% attapulgite by weight percentage Soil, 30% epoxy resin, 40% starch.
Embodiment 3
[0014] A kind of willow paint, made by the following components by weight: 25 parts of water-based acrylic resin, 40 parts of water, 15 parts of water-soluble alkyd paint, 3 parts of manganese dioxide, 8 parts of calcium stearate, 6 parts of three Glyceryl stearate, 18 parts of acrylic acid emulsion, 5 parts of sodium lauryl sulfonate, 8 parts of sodium metaphosphate, 4 parts of pentaerythritol, 4 parts of auxiliary agents, and the auxiliary agents are calculated as: 30% attapulgite by weight percentage Soil, 30% epoxy resin, 40% starch.
[0015] Select two batches of identical willows to adopt the willow paint of the present invention and ordinary paint to smear respectively, and track and count the effects after use.
[0016] Does it contain volatile substances such as benzene Leveling Drying time at 30°C Normal use time for the first paint drop Willow products that are often deformed in frequent use have a paint peeling time Willow paint of the pres...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com