[0019] Taisen product: choose 280g comprehensive quantification, 110g double tile composite, mix 1000kg water, 285kg cornstarch, 10kg caustic soda, 2.5kg borax, and 57kg tannin in the automatic glue making mixer for 45 minutes, check the viscosity for 17s, and form adhesive A , the two layers of core paper and between the core paper and the inner paper are bonded by adhesive A, and the gelatinization temperature is 60°C.
[0020] Stir 800kg of water, 285kg of cornstarch, 10kg of caustic soda, 2.8kg of borax, and 50kg of tannin in an automatic glue-making mixer for 45 minutes, check the viscosity for 20 seconds, and form adhesive B. The two layers of core paper and surface paper are bonded through adhesive B. The gelatinization temperature is 58-60°C.
Embodiment 2
[0022] Taisen product: choose 280g comprehensive quantitative, 110g double tile compound, mix 950kg water, 280kg cornstarch, 8kg caustic soda, borax 2kg, tannin 55kg in the automatic glue mixer for 45 minutes, check the viscosity for 17s to form adhesive A, The two layers of core paper and between the core paper and the inner paper are bonded by adhesive A, and the gelatinization temperature is 60°C.
[0023] Stir 750kg of water, 280kg of cornstarch, 8kg of caustic soda, 2.5kg of borax, and 48kg of tannin in an automatic glue-making mixer for 45 minutes, check the viscosity for 20 seconds, and form adhesive B. The two layers of core paper and surface paper are bonded through adhesive B. The gelatinization temperature is 58-60°C.
Embodiment 3
[0025] Taisen product: choose 280g comprehensive quantification, 110g double tile composite, mix 1050kg water, 290kg cornstarch, 12kg caustic soda, borax 3kg, tannin 58kg in the automatic glue mixer for 45 minutes, check the viscosity for 17s, and form adhesive A. The two layers of core paper and between the core paper and the inner paper are bonded by adhesive A, and the gelatinization temperature is 60°C.
[0026] Stir 850kg of water, 290kg of cornstarch, 12kg of caustic soda, 3.5kg of borax, and 52kg of tannin in an automatic glue-making mixer for 45 minutes, check the viscosity for 20 seconds, and form adhesive B. The two layers of core paper and surface paper are bonded through adhesive B. The gelatinization temperature is 58-60°C.
[0027] Adopt the glue formula of present embodiment, performance test is as follows:
[0028]
[0029] Note: The comprehensive quantitative of this product is 400g / m 2 , the comprehensive weight of five-layer corrugated cardboar...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com