A technology for autoclaving fly ash bricks and fly ash, which is applied in the field of building materials, can solve the problems of unsatisfactory performances such as compression resistance, bending resistance and freezing resistance, poor product strength, and inappropriate control of raw material component ratios, etc. problems, to achieve the effect of superior frost resistance and improved strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] The raw material components are as follows by weight percentage: 70% of fly ash, 17% of stone chips, 12% of lime, and 1% of gypsum. The weight percentage of active calcium oxide in the lime is 60%, and the weight percentage of silicon dioxide in the fly ash is 65%.
[0011] After testing, the autoclaved fly ash brick manufactured according to the raw material formula of this example has a thermal conductivity of 0.10W / m K, an average compressive strength greater than 25MPa, and an average flexural strength greater than 5Mpa, and its comprehensive performance is excellent. Applicable to similar products manufactured with traditional techniques and formulas.
Embodiment 2
[0013] The raw material components by weight percentage are: 60% of fly ash, 22% of stone chips, 15% of lime and 3% of gypsum. The weight percentage of active calcium oxide in the lime is 80%, and the weight percentage of silicon dioxide in the fly ash is 55%.
[0014] After testing, the autoclaved fly ash brick manufactured according to the raw material formula of this example has a thermal conductivity of 0.10W / m K, an average compressive strength greater than 25MPa, and an average flexural strength greater than 5Mpa, and its comprehensive performance is excellent. Applicable to similar products manufactured with traditional techniques and formulas.
Embodiment 3
[0016] The raw material components are as follows by weight percentage: 63% of fly ash, 20% of stone chips, 15% of lime and 2% of gypsum. The weight percentage of active calcium oxide in the lime is 70%, and the weight percentage of silicon dioxide in the fly ash is 60%.
[0017] After testing, the autoclaved fly ash brick manufactured according to the raw material formula of this example has a thermal conductivity of 0.10W / m K, an average compressive strength greater than 25MPa, and an average flexural strength greater than 5Mpa, and its comprehensive performance is excellent. Applicable to similar products manufactured with traditional techniques and formulas.
PUM
Property | Measurement | Unit |
---|---|---|
compressive strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com