Colorant composition and preparation method thereof
A composition and colorant technology, applied in the direction of coating, etc., can solve the problems of fast drying speed, unsuitable for large-area construction, and limited wide application
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0036] The invention provides a kind of preparation method of colorant composition, comprises the following steps:
[0037] Mix the water-based resin in parts by weight of the above technical solution with water, alcohol solvents, alcohol ether solvents, pH regulators, thickeners, and leveling agents to obtain agent A;
[0038] The agent A is mixed with the agent B to obtain a colorant composition; the agent B is a water-soluble color essence.
[0039] In the invention, the water-based resin is mixed with water, alcohol solvent, alcohol ether solvent, pH regulator, thickener and leveling agent to obtain agent A. In the present invention, the type and amount of the water-based resin, alcohol solvent, alcohol ether solvent, thickener, pH regulator, leveling agent and water are the same as those of the water-based resin, alcohol solvent, alcohol described in the above technical scheme. The types and amounts of ether solvents, thickeners, pH regulators, leveling agents and water ar...
Embodiment 1
[0065] Add 30 parts by weight of water-based alkyd resin and 19.5 parts by weight of water into the container, stir for 10 minutes at a stirring rate of 500 rpm, add 5 parts by weight of fumed silica, and stir at a stirring rate of 1500 rpm Stir for 5min, then add 15 parts by weight of ethylene glycol, 30 parts by weight of dipropylene glycol butyl ether, 0.3 parts by weight of BYK370 and AMP95 of 0.2 parts by weight, and stir for 10 minutes at a stirring rate of 1000 rpm to obtain A agent;
[0066] Place 38 parts by weight of red color essence, 60 weight parts of yellow color essence and 2 weight parts of black color essence in the container, and stir for 8 minutes at a stirring rate of 1000 rpm to obtain agent B;
[0067] The above-mentioned agent A and agent B are mixed to obtain a colorant composition.
[0068] The colorant composition obtained in Example 1 of the present invention is orange-brown.
[0069] The present invention tests the environmental protection, oil re...
Embodiment 2
[0077] Add 30 parts by weight of water-based vegetable oil and 19.5 parts by weight of water into the container, stir for 5 minutes at a stirring rate of 1000 rpm, add 5 parts by weight of fumed silica, and stir for 10 minutes at a stirring rate of 1200 rpm, followed by Add 15 parts by weight of ethylene glycol, 30 parts by weight of dipropylene glycol butyl ether, 0.3 parts by weight of BYK370 and 0.2 parts by weight of AMP95, and stir for 8 minutes at a stirring rate of 1000 rpm to obtain agent A;
[0078] Add 15 parts by weight of red color essence, 75 parts by weight of yellow color essence and 10 parts by weight of black color essence into the container, and stir at a stirring rate of 800 rpm for 10 minutes to obtain agent B;
[0079] The above-mentioned agent A and agent B are mixed to obtain a colorant composition.
[0080] The colorant composition obtained in Example 2 of the present invention is black walnut color.
[0081] The present invention tests the drying spee...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com