One-component laminating glue

A puzzle glue, one-component technology, applied in the direction of adhesive type, monocarboxylate copolymer adhesive, etc., can solve the problems of increasing the cost of use, short storage time of glue, easy to mix unevenly, etc., and achieve quality Guaranteed, less environmental pollution and easy to use

Inactive Publication Date: 2013-09-04
河北霖江木业有限公司
View PDF3 Cites 9 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

When the two-component glue is used, it needs to be temporarily blended in a specific proportion and stirred evenly, which leads to an extra process, increases th...

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0052] One-component puzzle glue of the present invention, its component comprises intermediate material, and the preparation method of described intermediate material is as follows:

[0053] 1) Raw material preparation:

[0054] The weight part is the vinyl acetate VAc of 400-430,

[0055] Parts by weight are 25-30 butyl acrylate BA,

[0056] Parts by weight are ethyl acrylate EA of 25-30,

[0057] Parts by weight are N-methylolacrylamide NMA of 14-20,

[0058] Parts by weight are vinyltrimethoxysilane of 0.5-1.5,

[0059] The weight part is the polyvinyl alcohol BP-05 of 7-13,

[0060] Parts by weight are polyvinyl alcohol BP-24 of 10-15,

[0061] Parts by weight are polyvinyl alcohol BP-17 of 34-38,

[0062] Parts by weight are the triethylamine of 0.5-1.5,

[0063] The weight part is the ammonium persulfate APS of 0.35-0.85,

[0064] Parts by weight are tertiary butyl hydroperoxide TBHP of 0.5-1.0,

[0065] Parts by weight are sodium formaldehyde sulfoxylate SFS o...

Embodiment 2

[0098] One-component puzzle glue of the present invention, its component comprises intermediate material, and the preparation method of described intermediate material is as follows:

[0099] 1) Raw material preparation:

[0100] 400 or 420 or 430 parts by weight of vinyl acetate VAc,

[0101] 25 or 27 or 30 parts by weight of butyl acrylate BA,

[0102] 25 or 27 or 30 parts by weight of ethyl acrylate EA,

[0103] 14 or 16 or 20 parts by weight of N-methylolacrylamide NMA,

[0104] Parts by weight are 0.5 or 1 or 1.5 vinyltrimethoxysilane,

[0105] Parts by weight are 7 or 10 or 13 polyvinyl alcohol BP-05,

[0106] Parts by weight are 10 or 12 or 15 polyvinyl alcohol BP-24,

[0107] Parts by weight are 34 or 36 or 38 polyvinyl alcohol BP-17,

[0108] Parts by weight are 0.5 or 1 or 1.5 triethylamine,

[0109] Parts by weight are 0.35 or 0.57 or 0.85 ammonium persulfate APS,

[0110] Parts by weight are 0.5 or 0.7 or 1.0 tert-butyl hydroperoxide TBHP,

[0111] Parts b...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention relates to a one-component laminating glue which comprises the following components in parts by weight: 900 to 945 parts of intermediate material, 25 to 30 parts of polyvinyl alcohol aqueous solution PVA-H2O with the weight percent concentration of 17%, 10 to 15 parts of AlCl3, 0.5 to 1.2 parts of mineral oil defoamer 691, 12 to 18 parts of multifunctional additive DB and 8 to 12 parts of plasticizer DPGDB (Dipropylene Glycol Dibenzoate), wherein the one-component laminating glue is formed by mixing all the components. The one-component laminating glue is very convenient to use, rapid in construction speed and low in cost. In addition, for the one-component laminating glue, the quality is further guaranteed; the heat-resistant performance is improved obviously; the service life and the open period are prolonged; and the one-component laminating glue generates little pollution to the environment.

Description

technical field [0001] The invention relates to a one-component puzzle glue. Background technique [0002] Panel glue refers to the adhesive used for splicing glulam and other wood products, and is suitable for panel bonding of non-structural materials and glulam for structural materials. At present, two-component splicing glue is commonly used in China. Two-component splicing glue means that in addition to glue, a curing agent is required to be used together. , to adjust to the appropriate ratio. When the two-component glue is used, it needs to be temporarily blended in a specific proportion and stirred evenly, which leads to an extra process, increases the cost of use, and is easy to mix unevenly, and gel appears during use. In addition, The storage time of the stirred glue is also relatively short (2 hours / 25°C or so). Contents of the invention [0003] In order to solve the above technical problems, the purpose of the present invention is to provide a kind of very c...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): C09J131/04C08F218/08C08F220/18C08F230/08C08F220/58
Inventor 宋立明
Owner 河北霖江木业有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products