Low-cost method for preparing nano calcium sulfate
A nano-calcium sulfate, low-cost technology, applied in the directions of nanotechnology, nanotechnology, calcium/strontium/barium sulfate, etc., can solve the problems of unfavorable industrial production and high cost of nano-calcium sulfate, and achieve high commercial value and low cost. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] A low-cost method for preparing nano-calcium sulfate, which comprises the following preparation steps in sequence:
[0025] Step A: refining sulfate-containing brine and calcium-containing brine, then mixing the refined sulfate-containing brine and calcium-containing brine, and stirring to form a mixed solution;
[0026] Step B: After the mixed solution obtained in step A is left to stand, add the precipitate at the bottom to a centrifuge, remove the mother liquor, add water to stir and wash, and then dehydrate with a centrifuge to obtain wet calcium sulfate dihydrate;
[0027] Step C: drying the wet calcium sulfate dihydrate obtained in step B at 101 degrees Celsius;
[0028] Step D: Grinding the dried calcium sulfate in step C with a nanoscale dispersing grinder to obtain nanoscale calcium sulfate.
[0029] Specifically, in the step A, when mixing the sulfate-containing brine and the calcium-containing brine, it is divided into three steps successively:
[0030] Ste...
Embodiment 2
[0034] A low-cost method for preparing nano-calcium sulfate, which comprises the following preparation steps in sequence:
[0035] Step A: refining sulfate-containing brine and calcium-containing brine, then mixing the refined sulfate-containing brine and calcium-containing brine, and stirring to form a mixed solution;
[0036] Step B: After the mixed solution obtained in Step A is left to stand, add the precipitate at the bottom to a plate-and-frame filter press for pressure filtration, and flush water while pressing to remove soluble impurities such as sodium chloride to obtain wet dihydrate Calcium sulfate;
[0037] Step C: drying the wet calcium sulfate dihydrate obtained in step B at 150 degrees Celsius;
[0038] Step D: Grinding the anhydrous calcium sulfate dried in step C with a nanoscale dispersing grinder to obtain nanoscale calcium sulfate.
[0039] Specifically, in the step A, when mixing the sulfate-containing brine and the calcium-containing brine, it is divide...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com