A technology for automobile exhaust and cleaning agent, which is used in fuel additives, petroleum industry, liquid carbon-containing fuels, etc., can solve the problems of inability to achieve good purification and small purification effect, and achieve the effects of low production cost, reduced pollution and simple preparation.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] Preparation:
[0023] (1) Preparation of Component A: Put 9g of ethyl propyl nitrate, 45g of ethylene glycol monomethyl ether, 20g of fatty alcohol and 60g of high-carbon fatty alcohol into a conical flask, mix well, and let it stand and age for 7-8 hours spare;
[0024] (2) Preparation of component B: Add 8g of N,N-dimethylacetamide, 40g of diisopropyl ether, 30g of lauryl alcohol, 2g of glycerol palm kernel fatty acid ester and 2.5g of glycerin oleic acid into a three-necked bottle in sequence, Heat it in a water bath under normal pressure to 50~53°C, and keep it warm for 4~6 hours;
[0025] (3) Refining 85g of polyhydric alcohol at 90~140℃ to make the water content less than 1%;
[0026] (4) Mix the prepared components A and B with the refined polyhydric crude alcohol, and leave to stand for 48 hours to obtain the finished product.
Embodiment 2
[0028] Preparation:
[0029] (1) Preparation of Component A: Put 8g of ethyl propyl nitrate, 40g of ethylene glycol monomethyl ether, 10g of fatty alcohol and 50g of high-carbon fatty alcohol into a conical flask, mix well, and let it stand and age for 7~8 hours spare;
[0030] (2) Preparation of component B: Add 7g of N,N-dimethylacetamide, 30g of diisopropyl ether, 20g of lauryl alcohol, 1g of glycerol palm kernel fatty acid ester and 2g of glycerin oleic acid into a three-necked bottle in turn, often Press down on the water bath and heat to 50~53°C, and keep it warm for 4~6 hours;
[0031] (3) Refining 82g of polyvalent crude alcohol at 90~140°C to make the water content less than 1%;
[0032] (4) Mix the prepared components A and B with the refined polyhydric crude alcohol, and leave to stand for 48 hours to obtain the finished product.
Embodiment 3
[0034] Preparation:
[0035] (1) Preparation of Component A: Put 1g of ethyl propyl nitrate, 50g of ethylene glycol monomethyl ether, 30g of fatty alcohol and 70g of high-carbon fatty alcohol into a conical flask, mix well, and let it stand and age for 7-8 hours spare;
[0036] (2) Preparation of component B: Add 10g of N,N-dimethylacetamide, 50g of diisopropyl ether, 40g of lauryl alcohol, 3g of glycerol palm kernel fatty acid ester and 3g of glycerin oleic acid into a three-necked bottle in sequence, often Press down on the water bath and heat to 50~53°C, and keep it warm for 4~6 hours;
[0037] (3) Refining 87g of polyvalent crude alcohol at 90~140°C to make the water content less than 1%;
[0038] (4) Mix the prepared components A and B with the refined polyhydric crude alcohol, and leave to stand for 48 hours to obtain the finished product.
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
dew point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com