A technology of latex paint and coating method for interior walls, used in antifouling/underwater coatings, devices for coating liquid on surfaces, coatings, etc. Cleaning, poor stain resistance, etc., to improve repairability, resist the penetration of stains and oil stains, and have good stain resistance and water resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0036] The steps for preparing the self-cleaning and decontaminating type interior wall latex paint of the present embodiment are as follows (the following are percentages by weight):
[0037] (1) At room temperature, add 35.75% pure water, 0.35% hydroxyethyl cellulose and 0.2% multifunctional additives into the mixing tank, and stir slowly for 5 to 10 minutes;
[0038] (2) After the hydroxyethyl cellulose is completely dissolved, add 0.15% defoamer, 0.5% wetting and dispersing agent, and 0.1% antiseptic and bactericide and stir for 3 to 5 minutes until uniform;
[0039] (3) Add 10% titanium dioxide pigment and 27.5% heavy calcium carbonate filler, stir and disperse at high speed for 15 to 20 minutes until the fineness is qualified (60μm), then add 2.5% nano decontamination factor and stir for 5 minutes ~ 10 minutes until uniform;
[0040] (4) Add 20% modified acrylic emulsion, 1.5% film-forming agent, 1.2% co-solvent, 0.15% defoamer and 0.1% leveling agent, stir and disperse...
Embodiment 2
[0049] The steps for preparing the self-cleaning and decontaminating type interior wall latex paint of the present embodiment are as follows (the following are percentages by weight):
[0050] (1) At room temperature, add 31.28% pure water, 0.42% hydroxyethyl cellulose and 0.2% multifunctional additives into the mixing tank, and stir slowly for 5 to 10 minutes;
[0051] (2) After the hydroxyethyl cellulose is completely dissolved, add 0.2% defoamer, 0.6% wetting and dispersing agent, and 0.15% antiseptic and bactericide, stir for 3 minutes to 5 minutes, and stir well;
[0052] (3) Add 15% titanium dioxide pigment and 20% heavy calcium carbonate filler, stir and disperse at high speed for 15 minutes to 20 minutes until the fineness is qualified (60μm), then add 3.5% nano decontamination factor and stir for 5 minutes to 10 minutes minutes, stir well;
[0053] (4) Add 25% modified acrylic emulsion, 1.8% film former, 1.5% co-solvent, 0.2% defoamer and 0.15 leveling agent, stir an...
Embodiment 3
[0056] The self-cleaning and decontaminating interior wall latex paints prepared in Examples 1 and 2 can be applied by brushing, roller coating and spraying.
[0057] When brushing the product of the present invention, add 10% to 15% of water (the total weight of the product), and after stirring evenly, it can be painted on a smooth and clean wall surface.
[0058] Use a short-haired roller for roller coating, and add 10% to 15% of water (total weight of the product).
[0059] Spraying can be done with air or airless spraying, only need to add about 10% (total weight of the product) of water to dilute and apply.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com