A technology of chitosan and therapeutic film, which is applied in the field of preparation of nano-iodine chitosan cervical therapeutic film and film, can solve the problems of affecting the curative effect, large dosage, drug and matrix outflow, etc., so as to promote wound healing and reduce discomfort Sensitive, improve the effect of bactericidal performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Film formulation:
[0020] Povidone-iodine 20g
[0021] Dioctyldimethylammonium chloride 1g
[0022] Chlorhexidine acetate 1g
[0023] Carboxymethyl Chitosan 30g
[0024] Hydroxypropyl Methyl Cellulose 40g
[0025] Glycerin 10g
[0026] Nano carbon fiber 2g
[0027] water 400mL
[0028] Add povidone iodine, dioctyldimethylammonium chloride and chlorhexidine acetate into appropriate amount of water, stir and heat at 80°C to dissolve, add carboxymethyl chitosan, hydroxypropyl methylcellulose, glycerin, Heat and stir at 80°C for 1 hour to dissolve and mix; cool down to 50°C and stir slowly, add adsorbent, continue to stir evenly, remove air bubbles, spread the board while it is hot, and dry at 60°C for 50 minutes. Filming, cutting.
Embodiment 2
[0030] Film formulation:
[0031] Povidone-iodine 15g
[0032] Didodecyldimethylammonium chloride 2g
[0033] Chlorhexidine acetate 2g
[0034] Carboxylated Chitosan 30g
[0035] Methylcellulose 40g
[0036] Glycerin 10g
[0037] Nano carbon fiber 3g
[0038] water 400mL
[0039] Add povidone iodine, didodecyldimethylammonium chloride and chlorhexidine acetate into an appropriate amount of water, stir and heat at 80°C to dissolve, add carboxylated chitosan, methylcellulose, glycerin, and dissolve at 80°C Heat and stir at ℃ for 1 hour to dissolve and mix; cool down to 50℃ and stir slowly, add adsorbent, continue to stir evenly, remove air bubbles, spread the board while it is hot, and dry at 60℃ for 50 minutes. Filming, cutting.
Embodiment 3
[0041] Film formulation:
[0042] Povidone-iodine 10g
[0043] Didecyldimethylammonium chloride 2g
[0044] Chlorhexidine acetate 2g
[0045] Carboxylated Chitosan 25g
[0046] Sodium Carboxymethyl Cellulose 45g
[0047] Sorbitol 10g
[0048] Nano carbon fiber 3g
[0049] water 500mL
[0050] Add povidone iodine, didecyldimethyl ammonium chloride and chlorhexidine acetate into appropriate amount of water, stir and heat at 80°C to dissolve them, add carboxylated chitosan, sodium carboxymethyl cellulose and sorbitol, Heat and stir at 80°C for 1 hour to dissolve and mix; cool down to 50°C and stir slowly, add adsorbent, continue to stir evenly, remove air bubbles, spread the board while it is hot, and dry at 60°C for 50 minutes. Filming, cutting.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com