Preliminary dip material for vacuum forming massive article
A large-scale product, vacuum forming technology, applied in the field of polymer materials, can solve the problems of reinforced fiber bending, unable to be discharged in time, and affecting the mechanical properties of the product
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0013] like figure 1 As shown, in this embodiment, after the epoxy resin composition is heated and melted, it is evenly coated on the release paper capable of carrying the resin so that the weight per unit area is 300g / m 2 resin film, and rolled up for use. Arrange the unidirectional carbon fiber bundles evenly so that the mass per unit area is 500g / m 2 , the coated resin film is bonded to the underside of the yarn bundle, and the resin is impregnated into the reinforcing fibers by heating and / or pressure, so that the matrix resin is completely impregnated into one side of the reinforcing fibers, forming a reinforcing fiber that is completely saturated with the matrix resin 3 , and control that the other side of the reinforcing fiber cannot be completely saturated with the resin, forming a reinforcing fiber 2 that is not completely saturated with the matrix resin, the impregnation rate is controlled at 80%, and a prepreg is formed, and then the weight per unit area is 25g / m ...
Embodiment 2
[0014] Embodiment 2: After the epoxy resin composition is heated and melted, it is evenly coated on the release paper so that the weight per unit area is 320g / m 2 resin film, and rolled up for use. Evenly arrange the glass fibers so that the mass per unit area is 600g / m 2 , the coated resin film is attached to the bottom of the fiber, and the resin is impregnated into the fiber by heating and pressing, so that the lower surface of the reinforcing fiber is completely saturated with the matrix resin, and the upper surface of the fiber is controlled not to be completely saturated with the resin. The impregnation rate is controlled as 90%, and then the weight per unit area is 6g / m 2 The triaxial polyamide mesh is flatly attached to the side that is not completely saturated with resin, and the yarn used in the triaxial polyamide mesh is selected from 12Tex mesh. The spacing is 25mm.
Embodiment 3
[0015] Example 3: In this example, after the epoxy resin composition is heated and melted, it is evenly coated on the release paper capable of carrying the resin so that the weight per unit area is 550g / m 2 resin film, and rolled up for use. The coated resin film with a unit area of 900g / m 2 The underside of the triaxial stitchbonded fabric is laminated, and the resin is impregnated into the reinforcing fiber by heating and / or pressure, so that the matrix resin is completely impregnated into one side of the reinforcing fiber, forming a reinforcing fiber 3 completely saturated with the matrix resin, and controlling the reinforcement The other side of the fiber cannot be completely impregnated with the resin, forming a reinforcing fiber 2 in which the matrix resin is not completely impregnated, and the impregnation rate is controlled at 70% to form a prepreg.
[0016] When utilizing the present invention to manufacture large-scale plate products, one side of the reinforcing f...
PUM
Property | Measurement | Unit |
---|---|---|
gel time | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com