Ageing resistance composite modifying agent for bitumen for road use
A composite modifier and anti-aging technology, applied in the field of materials, can solve the problem of not improving the anti-aging performance of asphalt, and achieve the effects of improving its own performance, improving durability, and slowing down the speed and degree of aging.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] Taking the production of product 100kg of the present invention as an example, the raw materials used and their weight proportions are:
[0030] Antiaging agent 2246-S 18.75kg
[0031] Antioxidant 168 18.75kg
[0032] Carbon black DL8 62.5kg
[0033] The proportioning by weight of above-mentioned raw material is:
[0034] Antiaging agent 2246-S 0.6 parts
[0035] Antioxidant 168 0.6 parts
[0036] Carbon black DL8 2 parts
[0037] Its preparation method is as follows:
[0038] Put anti-aging agent 2246-S, antioxidant 168, and carbon black DL8 into a stainless steel bucket, stir it with a high-speed shearer for 5 to 10 minutes to make it fully mixed, and make the asphalt anti-aging composite modifier for road use of the present invention. Subpackage.
Embodiment 2
[0040] Taking the production of product 100kg of the present invention as an example, the raw materials used and their weight proportions are:
[0041] Antiaging agent 2246-S 23.68kg
[0042] Antioxidant 168 23.68kg
[0043] Carbon black DL8 52.64kg
[0044] The proportioning by weight of above-mentioned raw material is:
[0045] Antiaging agent 2246-S 0.9 parts
[0046] Antioxidant 168 0.9 parts
[0047] Carbon black DL8 2 parts
[0048] Its preparation method is identical with embodiment 1.
Embodiment 3
[0050] Taking the production of product 100kg of the present invention as an example, the raw materials used and their weight proportions are:
[0051] Antiaging agent 2246-S 22.22kg
[0052] Antioxidant 168 22.22kg
[0053] Carbon black DL8 55.56kg
[0054] The proportioning by weight of above-mentioned raw material is:
[0055] Antiaging agent 2246-S 0.8 parts
[0056] Antioxidant 168 0.8 parts
[0057] Carbon black DL8 2 parts
[0058] Its preparation method is identical with embodiment 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com