Method of supporting along spatially keeping lane end
A support method and composite admixture technology, applied in the direction of pillars/supports, fillings, safety devices, etc., can solve the problems of violent surrounding rock activities in the roadway, difficulty in maintaining the stability of the roadway, and difficult maintenance of the roadway, so as to prevent spontaneous combustion , reduce pressure and maintain stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0046] 1. Preparation
[0047] Cement, fly ash, gravel, sand and water, the amount of each component is by weight:
[0048] 14 parts of cement and 20 parts of fly ash
[0049] 28 parts of stone, 22 parts of sand, 16 parts of water
[0050] The content of the effective components of the composite admixture is 1.3% of the total amount of cement and fly ash by weight percentage.
[0051] The composition of used composite admixture is by weight:
[0052] 30 parts of polycarboxylic acid as water reducing agent,
[0053] Carboxymethylcellulose as a water-retaining agent is 1.5 parts,
[0054] Rosin thermopolymer as air-entraining agent is 1.2 parts,
[0055] Calcium chloride as an early strength agent is 67.3 parts.
[0056] The cement, fly ash, gravel and sand used are:
[0057] Cement: P.042.5 grade, fly ash: II grade, stone: maximum particle size: 6mm, sand: medium sand.
[0058] 2. Construction process
[0059] Cement, fly ash, gravel, sand and composite admixtures are ...
Embodiment 2
[0065] 1. Ingredients
[0066] Cement, fly ash, gravel, sand and water, the amount of each component is by weight:
[0067] 20 parts of cement and 7 parts of fly ash
[0068] 40 parts of gravel, 20 parts of sand, 13 parts of water
[0069] The active ingredient content of the composite admixture is 1.6% by weight of the total amount of cement and fly ash.
[0070] The composition of used composite admixture is by weight percentage:
[0071] 30 parts of polycarboxylic acid as water reducing agent,
[0072] Carboxymethylcellulose as a water-retaining agent is 1.5 parts,
[0073] Rosin thermopolymer as air-entraining agent is 1.2 parts,
[0074] Calcium chloride as an early strength agent is 67.3 parts.
[0075] The cement, fly ash, gravel and sand used are:
[0076] Cement: P.042.5 grade, fly ash: II grade, stone: maximum particle size: 6mm, sand: medium sand
[0077] Two, construction process is the same as embodiment 1
[0078] 3. Product performance:
[0079] 1. The...
Embodiment 3
[0083] 1. Preparation
[0084] Cement, fly ash, gravel, sand and water, the amount of each component is by weight:
[0085] 10 parts of cement and 40 parts of fly ash
[0086] 15 parts of stone, 15 parts of sand, 20 parts of water
[0087] The content of the effective components of the composite admixture is 1.5% of the total amount of cement and fly ash by weight percentage.
[0088] The composition of used composite admixture is by weight:
[0089] 30 parts of polycarboxylic acid as water reducing agent,
[0090] Carboxymethylcellulose as a water-retaining agent is 1.5 parts,
[0091] Rosin thermopolymer as air-entraining agent is 1.2 parts,
[0092] Calcium chloride as an early strength agent is 67.3 parts.
[0093] The cement, fly ash, gravel and sand used are:
[0094] Cement: P.042.5 grade, fly ash: II grade, stone: maximum particle size: 6mm, sand: medium sand
[0095] Two, construction process is the same as embodiment 1
[0096] 3. Product performance:
[00...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com