Concrete member water-washed chiseling process
A technology of concrete and technology, which is applied in the field of water flushing and chiseling of concrete components, can solve the problems of high construction strength, time-consuming and laborious chisel quality, and insufficient chisel quality, so as to ensure the firmness of the bond, save labor and time, and improve The effect of construction efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0069] A kind of water flushing chiseling process for concrete members, comprising the steps of:
[0070] S1: bottom tire treatment
[0071] Check the bottom tire to ensure that the surface of the bottom tire is smooth and clean, the sidelines are straight and free of pits, the rubber strips on both sides of the bottom tire are intact, and there is no slag between the rubber strip and the bottom tire. The iron surface on both sides of the bottom tire surface should be Ensure smoothness and tight fit with the wooden square, ensure that the iron sheet does not bulge, and there is no ash under the iron sheet and the wooden square. When there is ash on the bottom tire, local settlement, cracking, rubber strip damage, iron sheet damage, and ash inclusions, Repair or replace the bottom tire;
[0072] S2: Apply release agent
[0073] Apply release agent evenly on the treated bottom tire, the release agent should not be too thick, to avoid oil accumulation on the bottom tire, so as ...
Embodiment 2
[0099] A kind of water flushing chiseling process for concrete members, comprising the steps of:
[0100] S1: bottom tire treatment
[0101] Check the bottom tire to ensure that the surface of the bottom tire is smooth and clean, the sidelines are straight and free of pits, the rubber strips on both sides of the bottom tire are intact, and there is no slag between the rubber strip and the bottom tire. The iron surface on both sides of the bottom tire surface should be Ensure smoothness and tight fit with the wooden square, ensure that the iron sheet does not bulge, and there is no ash under the iron sheet and the wooden square. When there is ash on the bottom tire, local settlement, cracking, rubber strip damage, iron sheet damage, and ash inclusions, Repair or replace the bottom tire;
[0102] S2: Apply release agent
[0103] Apply release agent evenly on the treated bottom tire, the release agent should not be too thick, to avoid oil accumulation on the bottom tire, so as ...
Embodiment 3
[0129] A kind of water flushing chiseling process for concrete members, comprising the steps of:
[0130] S1: bottom tire treatment
[0131] Check the bottom tire to ensure that the surface of the bottom tire is smooth and clean, the sidelines are straight and free of pits, the rubber strips on both sides of the bottom tire are intact, and there is no slag between the rubber strip and the bottom tire. The iron surface on both sides of the bottom tire surface should be Ensure smoothness and tight fit with the wooden square, ensure that the iron sheet does not bulge, and there is no ash under the iron sheet and the wooden square. When there is ash on the bottom tire, local settlement, cracking, rubber strip damage, iron sheet damage, and ash inclusions, Repair or replace the bottom tire;
[0132] S2: Apply release agent
[0133] Apply release agent evenly on the treated bottom tire, the release agent should not be too thick, to avoid oil accumulation on the bottom tire, so as ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com