A technology of collapsible loess and a treatment method, which is applied in the field of improving the treatment of collapsible loess foundation, can solve the problem of settlement that is not well solved, the problem of under-compaction of foundation soil is uneven, backfilling and compacting loess compaction Insufficient degree and other problems, to achieve the effect of controlling uneven settlement, short curing time and fast curing rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] Embodiment 1: a kind of processing method of improving collapsible loess foundation, comprises the following steps:
[0030] (1) Crushing and refining the loess;
[0031] (2) Evenly mix the pulverized loess and sodium silicate at a dry mass ratio of 100:10;
[0032] (3) Adjust the moisture content range of the mixture to 3%, and then carry out filling;
[0033] (4) Apply an AC electric field to the mixture, the electric field strength is 100V / m, and the electrification time is 0.5 hours;
[0034] (5) Curing the mixture after electric field treatment for 24 hours.
Embodiment 2
[0035] Embodiment 2: a kind of processing method of improving collapsible loess foundation, comprises the following steps:
[0036] (1) Crushing and refining the loess;
[0037] (2) Evenly mix the pulverized and refined loess and potassium silicate at a dry mass ratio of 100:0.5;
[0038] (3) Adjust the moisture content range of the mixture to 20%, and then carry out filling;
[0039] (4) Apply an AC electric field to the mixture, the electric field strength is 500V / m, and the electrification time is 0.2 hours;
[0040] (5) Curing the mixture after electric field treatment for 48 hours.
Embodiment 3
[0041] Embodiment 3: a kind of processing method of improving collapsible loess foundation, comprises the following steps:
[0042] (1) Crushing and refining the loess;
[0043] (2) Evenly mix crushed and refined loess, sodium silicate, and potassium silicate in a dry mass ratio of 100:0.5:0.5;
[0044] (3) Adjust the moisture content range of the mixture to 10%, and then carry out filling;
[0045] (4) Apply an AC electric field to the mixture, the electric field strength is 200V / m, and the electrification time is 0.3 hours;
[0046] (5) Curing the mixture after electric field treatment for 72 hours.
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
density | aaaaa | aaaaa |
density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com