Clivia soilless culture substrate and producing method thereof
The technology of a soilless cultivation substrate and a production method is applied in the field of Clivia soilless cultivation substrate and its production, which can solve the problems of low planting survival rate and achieve the effects of high water content, strong moisture retention, and promotion of growth and development
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] Take 20 kg of peat and sterilize it at high temperature for 2 hours, take it out and dry it in the sun for 48 hours; take 10 kg of willow bark with a length of 4 mm and a thickness of 1 mm, soak it in 0.5 kg of lime water for 24 hours, then sterilize it at high temperature for 2 hours, take it out Afterwards, dry and expose to the sun for 48 hours; mix 20 kg of treated peat, 10 kg of willow bark, and 6 kg of perlite, add 4 kg of clear water and stir until uniform; take 10 kg of the above-mentioned uniformly mixed raw materials, and then add 0.0067 kg of seaweed Fertilizer, mixed and stirred for 30 minutes until uniform, that is, the matrix was obtained, and it was bagged for later use.
Embodiment 2
[0018] Take 20 kg of peat and sterilize it at high temperature for 2 hours, take it out and dry it in the sun for 60 hours; take 10 kg of willow bark with a length of 6 mm and a thickness of 1 mm, soak it in 0.5 kg of lime water for 24 hours, then sterilize it at high temperature for 2 hours, take it out Afterwards, dry and expose to the sun for 60 hours; mix 20 kg of peat after treatment, 10 kg of willow bark, and 6 kg of perlite, add 4 kg of clear water and stir until uniform; take 10 kg of the above-mentioned uniformly mixed raw materials, and then add 0.0067 kg of seaweed Fertilizer, mixed and stirred for 30 minutes until uniform, that is, the matrix was obtained, and it was bagged for later use.
Embodiment 3
[0020] Take 20 kg of peat and sterilize at high temperature for 2 hours, take it out and dry it in the sun for 72 hours; take 10 kg of willow bark with a length of 8 mm and a thickness of 2 mm, soak it in 0.5 kg of lime water for 24 hours, then sterilize it at high temperature for 2 hours, take it out Afterwards, dry and expose to the sun for 72 hours; mix 20 kg of treated peat, 10 kg of willow bark, and 6 kg of perlite, add 4 kg of clear water and stir until uniform; take 10 kg of the above-mentioned uniformly mixed raw materials, and then add 0.0067 kg of seaweed Fertilizer, mixed and stirred for 30 minutes until uniform, that is, the matrix was obtained, and it was bagged for later use.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com