Gold-silver colour product and making method
A manufacturing method, gold and silver color technology, applied in the direction of metal layered products, chemical instruments and methods, layered products, etc., can solve the problems of high cost and single color, and achieve low cost, bright color without dullness, and good quality Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] Embodiment 1, the surface of the base material 11 with a thickness of 10 μm to 1 mm is plated with gold or covered with a hot stamping film, and hot stamping paper is used, and the predetermined pattern and identification mark are input into the film according to the ratio of 1:1, and the pattern on the film is printed to the film. On the surface of the resin plate and the metal plate, according to the material of the base material, the pressing temperature of the plastic type is controlled within 50-250°C, and the pressing temperature of the paper type is controlled within 20-140°C, and then according to the thickness of the base material 11 According to the depth of the molding groove 13 to be pressed, the total time of hot pressing and cooling is controlled within 5-60s.
[0036] The plate 1 with the golden surface is placed between resin plates or metal plates with concave-convex patterns on the surface, and press-molded according to the set pressure, temperature and...
Embodiment 2
[0038] Embodiment 2, the surface of the base material 11 with a thickness of 10 μm to 1 mm is plated with gold, covered with bronzing film or bronzing paper, the predetermined pattern and identification mark are input into the film according to the ratio of 1:1, and the pattern on the film is printed to the film. On the surface of the resin plate and the metal plate, according to the material of the base material, the pressing temperature of the plastic type is controlled within 50-250°C, and the pressing temperature of the paper type is controlled within 20-140°C, and then according to the thickness of the base material 11 According to the depth of the molding groove 13 to be pressed, the total time of hot pressing and cooling is controlled within 5-60s.
[0039] The plate 1 with the golden surface is placed between resin plates or metal plates with concave-convex patterns on the surface, and press-molded according to the set pressure, temperature and time.
[0040] The surfa...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
temperature | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com