Technology of aging wooden products
A process method and wood product technology, which is applied in the field of wood product aging treatment, can solve the problems of not achieving the wood carbonization process effect, unsatisfactory wood product covering effect, difficult time and temperature control, etc., to achieve good color levels, Highlight the effect of engraving and low cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0005] Embodiment 1, the process of making old wood products is achieved through the following process steps: first put 1200 g of potassium permanganate oxidant in the container, dilute with 20 liters of water, and control the water temperature between 30 ° C and 50 ° C. It melts and stirs well, then puts the processed wood product in the container, soaks it for 2-5 minutes, then takes the wood product out of the container, at this time, the surface of the oxidized wood product presents the effect of wood charring; after 5-10 hours After the wood products are naturally dried, they are made into various furniture, and then sanded, polished, and painted.
Embodiment 2
[0006] Embodiment 2, the process method of making old wooden decorative panels is realized by the following process steps: first put 1000g of potassium permanganate oxidant in the container, dilute it with 15 liters of water and make it melt and stir well, the water temperature is controlled at 30 Between ℃ and 50℃, put the processed wood products in the container, soak for 2 to 5 minutes and then take out the wood products from the container. At this time, the surface of the oxidized wood products shows the effect of wood charring; after 5~ After 10 hours of natural drying of the wood products, sanding, polishing and painting can be carried out.
Embodiment 3
[0007] Embodiment 3, the process method of woodcarving handicraft making old is realized by the following process steps: first put 800g of potassium permanganate oxidizing agent in the container, dilute it with 10 liters of water and make it melt and stir well, the water temperature is controlled at 30 ℃~ Between 50°C, put the processed wood products in the container, soak for 2 to 5 minutes and then take out the wood products from the container. At this time, the surface of the oxidized wood products shows the effect of wood charring; after 5 to 10 hours After the wood products are dried naturally, they can be sanded, polished and painted.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com