An acquisition method and impurity technology are applied in the field of obtaining the impurity rate of crushed scrap steel, which can solve the problems affecting the use of crushed scrap steel, inclusion of impurities and harmful substances, and achieve the effect of saving time and easy selection and avoiding difficulty in selection.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0055] This embodiment provides a method for obtaining the impurity rate of broken steel scrap, which is to sample and measure a naturally piled scrap pile, the mass of which is 40 tons. The method for obtaining the impurity ratio of broken steel scrap includes the following steps:
[0056] Use a forklift to suck out or push out a section of the natural pile as a sampling surface; 5.2kg of samples are collected at the four sampling points at the upper end, lower end, left end and right end of the sampling surface.
[0057] After mixing the samples from the four sampling points, use a sieve with a sieve aperture of 2.0mm for screening, and select the impurities in the under-sieve and the impurities in the over-sieve to obtain the total amount of impurities.
[0058] figure 1 The picture of the undersize impurity of the present embodiment is shown;
[0059] figure 2 Show the picture of this embodiment qualified material;
[0060] image 3 A picture of the oversize picked o...
Embodiment 2
[0065] This embodiment provides a method for obtaining the impurity rate of broken steel scrap, which is to sample and measure a naturally piled scrap pile, the mass of which is 40 tons. The method for obtaining the impurity ratio of broken steel scrap includes the following steps:
[0066] Use a forklift to suck out or push out a section of the natural pile as a sampling surface; 6.67kg of samples are collected at the four sampling points at the upper end, lower end, left end and right end of the sampling surface.
[0067] After mixing the samples from the four sampling points, use a sieve with a sieve aperture of 2.2 mm for screening, and select the impurities in the under-sieve and the impurities in the over-sieve to obtain the total amount of impurities.
[0068] The quality of the impurities under the sieve was weighed by a weighing device with a weighing accuracy of 1g to be 187g; the quality of the selected impurities was weighed by a weighing device with a weighing acc...
Embodiment 3
[0071] This embodiment provides a method for obtaining the impurity rate of broken steel scrap, which is to sample and measure a naturally piled scrap pile, the mass of which is 40 tons. The method for obtaining the impurity ratio of broken steel scrap includes the following steps:
[0072] Use a forklift to suck out or push out a section of the natural pile as a sampling surface; 5.2kg of samples are collected at the four sampling points at the upper end, lower end, left end and right end of the sampling surface.
[0073] After mixing the samples from the four sampling points, use a sieve with a sieve aperture of 1.8 mm for screening, and select the impurities in the under-sieve and the impurities in the over-sieve to obtain the total amount of impurities.
[0074] The quality of the impurities under the sieve was weighed by a weighing device with a weighing accuracy of 1g to be 152g; the quality of the selected impurities was weighed by a weighing device with a weighing accu...
PUM
Property | Measurement | Unit |
---|---|---|
Height | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com