A composition and pigment technology, applied in the directions of pigment slurry, color measuring device, device for coating liquid on the surface, etc., can solve problems such as inability to precisely control, achieve small color difference, high weather resistance and stability, accurate high degree of effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] Weigh 8.41 grams of PY74, 4.2 grams of PR101, 0.49 grams of PBK7, 17.82 grams of PW6, and 1000 grams of CSC-B base material. Mix the above materials evenly, and then apply the obtained composition on the substrate evenly and evenly by mechanical coating under the conditions of relative humidity of 50%±5% and room temperature of 23±2°C. It is a metal material or a non-metal material. The wet film thickness of the coating is 250 μm, and then placed in a precision oven at 50 ± 2 ° C for 3 to 4 hours to a constant weight, taken out, cooled to room temperature, and obtained color characterization.
Embodiment 2
[0026] Weigh 8.41 grams of PY74, 4.2 grams of PR101, 0.49 grams of PBK7, 17.6 grams of PW6, and 1000 grams of CSC-C base material. Manufacturing process is with embodiment 1.
Embodiment 3
[0028] Weigh 8.41 grams of PY74, 4.2 grams of PR101, 0.49 grams of PBK7, 18.0 grams of PW6, and 1005 grams of CSC-C base material. Manufacturing process is with embodiment 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com