Embodiment 1
[0030] Example 1: Utilizing waste lubricating oil to prepare regenerated base oil
[0031] The first waste No. 32 anti-wear hydraulic oil (L-HM32) has a yellowish-brown color, becomes turbid with water, and has obvious sour odor after oxidation. Treated by the following process:
[0032] Step A, preparation of chemical solution: preparation containing NaOH mass concentration is 3%, NaOH 2 SO 3 Mass concentration 5%, CH 3 CH 2 OH mass concentration of 5% aqueous solution.
[0033] Step B, after the waste lubricating oil to be treated is adsorbed and filtered through a mineral fiber filter, material a is obtained;
[0034] Step C, pumping the material a into a refining tank, stirring, and heating the material a at the same time;
[0035] Step D, fully reacting the material a and the chemical solution in the refining tank; the specific steps of the reaction include: ① When the temperature of the refining tank rises to 60-70 ° C, the chemical solution prepared in the step A T...
Embodiment 2
[0045] Embodiment 2 prepares nanometer novel metal processing oil
[0046] Step 1, pump the regenerated base oil prepared in Example 1 into a vacuum air conditioner and kettle, start stirring, start the vacuum system, and heat the regenerated base oil at the same time;
[0047] Step 2: Fully mix the regenerated base oil with the nano-extreme pressure anti-wear agent, and disperse evenly; the specific reaction steps include: ①Heating the regenerated base oil in the vacuum reactor at a stirring speed of 90 rpm to 60- Dehydration, degassing, deodorization and deodorization at 70°C and vacuum degree ≥ 0.09Mpa for about 0.5 hours; Pump in the required nano-extreme pressure anti-wear agent; ③Keep the oil temperature in the vacuum reactor at 60-70°C, the stirring speed at 90 rpm, and the vacuum degree ≥ 0.09Mpa for 1 hour to obtain the crude product of nano-new metal processing oil ;
[0048] Step 3: After the crude product of the nano new metal processing oil obtained in the above...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com