A new and old concrete, fine stone concrete technology, applied in the direction of adhesive types, building material processing, ester copolymer adhesives, etc., can solve the problems of difficult driving, large capital consumption, long construction time, etc., and achieve penetration Strong, good fluidity, cost-saving effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] In the process of pouring 600mm×600mm columns, the concrete pouring is interrupted for some reason, and it has been 5 hours since the pouring can be resumed, exceeding the initial setting time of the concrete, and the following methods are used to deal with it:
[0019] 1. Production of treatment agent: 10kg of cyclohexene, 20kg of methyl acrylate, 25kg of IC type finish oil produced by Kunming Building Waterproof Material Factory, 12kg of nonylphenol polyoxyethylene (10) ether, fatty alcohol polyoxyethylene (15 ) ether 6kg. Production method: Mix cyclohexene and methyl acrylate in proportion, stir at 30°C under normal pressure for 6 hours, then add IC type finish oil produced by Kunming Building Waterproof Material Factory, nonylphenol polyoxyethylene ( 10) Ether, fatty alcohol polyoxyethylene (15) ether, stirred under normal pressure at a temperature of 30° C. for 4 hours to obtain a milky white liquid.
[0020] Second, the construction steps to realize the bonding o...
Embodiment 2
[0024] Road new and old concrete pavement bonding treatment.
[0025] 1. Production of treatment agent: 20kg of cyclohexene, 35kg of butyl acrylate, 40kg of IC type finish oil produced by Kunming Building Waterproof Material Factory, 22kg of nonylphenol polyoxyethylene (10) ether, fatty alcohol polyoxyethylene (15 ) ether 15kg. Production method: Mix cyclohexene and butyl acrylate in proportion, stir at 15°C under normal pressure for 8 hours, then add IC type finish oil produced by Kunming Building Waterproof Material Factory, nonylphenol polyoxyethylene ( 10) Ether, fatty alcohol polyoxyethylene (15) ether, stirred under normal pressure at a temperature of 15° C. for 6 hours to obtain a milky white liquid.
[0026] Second, the construction steps to realize the bonding of new and old concrete:
[0027] ① Mix the above-mentioned treatment agent into the stirred concrete and stir evenly, treatment agent: mixed concrete = 1:100; ② Apply the treatment agent to the joints of the ...
Embodiment 3
[0030] During the pouring process of the building slab, the concrete pouring is interrupted for some reason, and the initial setting time of the concrete has passed when the pouring can be resumed, and the following methods are used to deal with it:
[0031] 1. Production of treatment agent: 17kg of cyclohexene, 30kg of butyl acrylate, 35kg of IC type finish oil produced by Kunming Building Waterproof Material Factory, 18kg of nonylphenol polyoxyethylene (10) ether, fatty alcohol polyoxyethylene (15 ) ether 12kg. Production method: Mix cyclohexene and butyl acrylate in proportion, stir at 25°C under normal pressure for 6 hours, then add IC type finish oil produced by Kunming Building Waterproof Material Factory, nonylphenol polyoxyethylene ( 10) Ether, fatty alcohol polyoxyethylene (15) ether, stirred under normal pressure at a temperature of 25° C. for 5 hours to obtain a milky white liquid.
[0032] Second, the construction steps to realize the bonding of new and old concre...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com